Thread: Welding question

  1. #1

    Default Welding question

    I am trying to fill in a threaded section on a tube. Picture a 6" piece of steel pipe. 14mm threaded hole on 1 end and a 3/8" hole on the other. I want to fill in the 14mm hole so I can drill and re tap it 1/2". But I do not want to fill the whole pipe in.

    I was thinking putting a piece of 3/8" brass or aluminum in the end to keep the weld from filling in. Thinking the weld won't stick to a non ferrous metal. BTW the pipe is steel.

    Other ideas???
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  2. Default

    Quote Originally Posted by Brian Ski View Post
    I am trying to fill in a threaded section on a tube. Picture a 6" piece of steel pipe. 14mm threaded hole on 1 end and a 3/8" hole on the other. I want to fill in the 14mm hole so I can drill and re tap it 1/2". But I do not want to fill the whole pipe in.

    I was thinking putting a piece of 3/8" brass or aluminum in the end to keep the weld from filling in. Thinking the weld won't stick to a non ferrous metal. BTW the pipe is steel.

    Other ideas???
    when you talk pipe you should give the schedule and size. when i first saw the six inch i thought it must be six inch pipe of unknown schedule; not length. it appears the ends are capped but who knows. you could take a bolt that fits the 14 mm hole insert/cut, weld perimeter, center punch and redrill.

    or you could tap for 5/8ths unc/unf
    Last edited by fdcmiami; 12-26-2012 at 12:30 PM.

  3. Default

    there is also a difference between tube and pipe; two different animals. so now i am thinking this is a piece of tube that has an id on one that accepted a 14 mm tap but wait. what about the other end? it's only 3/8ths. hmmm how does that work. oh, maybe the holes are not on the end but on the body of the tube/pipe itself. hmmm put a camera on next years christmas list.

    signed.
    grinch

  4. #4

    Default

    Quote Originally Posted by Brian Ski View Post
    I am trying to fill in a threaded section on a tube. Picture a 6" piece of steel pipe. 14mm threaded hole on 1 end and a 3/8" hole on the other. I want to fill in the 14mm hole so I can drill and re tap it 1/2". But I do not want to fill the whole pipe in.

    I was thinking putting a piece of 3/8" brass or aluminum in the end to keep the weld from filling in. Thinking the weld won't stick to a non ferrous metal. BTW the pipe is steel.

    Other ideas???
    I have only done something like this teh other way around. I had to fill a threaded piece of AL. The other difference was that my piece was only 9 inches long of 5/16 thick 1.5" pipe. I used a piece of steel to help with the fill.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  5. #5
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by fdcmiami View Post
    there is also a difference between tube and pipe; two different animals. so now i am thinking this is a piece of tube that has an id on one that accepted a 14 mm tap but wait. what about the other end? it's only 3/8ths. hmmm how does that work. oh, maybe the holes are not on the end but on the body of the tube/pipe itself. hmmm put a camera on next years christmas list.

    signed.
    grinch
    I agree, I have no idea what you are talking about. But weld will not stick to copper or thick aluminum so you can use them for a backing.
    Long arc, short arc, heliarc and in-the-dark!

  6. #6

    Default

    Quote Originally Posted by fdcmiami View Post
    when you talk pipe you should give the schedule and size. when i first saw the six inch i thought it must be six inch pipe of unknown schedule; not length. it appears the ends are capped but who knows. you could take a bolt that fits the 14 mm hole insert/cut, weld perimeter, center punch and redrill.

    or you could tap for 5/8ths unc/unf
    Sorry... Trying to run the question up the flag pole before work so I was in a hurry. This part is like a hollow, short, metal, table leg.

    I guess the best way to describe without a picture is a piece of 1/2" id steel pipe about 6" long. (similar to galvanized water pipe.) I think it is about a 1" od. Wall thickness is about 1/8". Got a taper to it so the non threaded end is about 3/8" id.

    Good idea of using a bolt except this is a 14 mm with a left handed. I want to get rid of the bastard size and convert it over to 1/2".

    I guess I could just hit the end with the mig welder and fill it in, but was looking for something that would give it a better flatter weld on the inside. Instead of gobs of weld.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  7. #7

    Default

    Get a heavier grade 8 flat washer 1/4" or 5/16" size weld it to the end of the pipe trim off the excess and re thread it to the size you want.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

Similar Threads

  1. Spot welding question.
    By Brian Ski in forum General Welder Questions
    Replies: 19
    Last Post: 08-18-2014, 12:02 PM
  2. tig welding question
    By steve1989 in forum General Welding Questions
    Replies: 3
    Last Post: 07-31-2013, 04:03 PM
  3. Tube welding question
    By agent4573 in forum General Welding Questions
    Replies: 8
    Last Post: 04-06-2013, 12:01 PM
  4. Welding helmet question
    By Brian Ski in forum General Welding Questions
    Replies: 43
    Last Post: 05-17-2012, 02:22 PM
  5. practice welding question
    By Brian Ski in forum General Welding Questions
    Replies: 22
    Last Post: 05-04-2012, 10:33 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •