    Neighbor borrowed a portaband blade this morning, when he came to bring it back, he also had his old portaband in his hand. Frayed cord, wheels all wobbly, bottom corner broken off (like so many of them are...) and generally a sad piece of tool.

    Well, I figured I'd take a look at it since he GAVE it to me. 15 minutes and I had fixed the problem with the wheels, identified three other issues and will be repairing them, I have a new cord and the motor is in great shape. I need to buy two new tires and some brushes, but I'm rebuilding the whole thing, getting rid of the gunk and grime, shine it up like new and get another 30 years out of it.

    So the main thing, is it a straight aluminum alloy casting? Anyone welded one up before? I'm going to have to graft a piece of AL in place, the plan was to build a few beads on the broken edge, then make a piece to fit, weld it in and grind it smooth/clearance the inside.

    Forgot to mention, sorry, it's a Milwaukee.
    Last edited by Trip59; 12-24-2012 at 12:53 AM. Reason: forgot manufacturer
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  2. #2

    Default

    Sounds like a nice project for the contest. Lots of pictures please.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. #3
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Quote Originally Posted by zoama585 View Post
    Sounds like a nice project for the contest. Lots of pictures please.
    Already have one for that category, but yeah, there will be lots of pictures. Unfortunately, I didn't think to take one as it sat when he gave it to me, but I'm snapping pics along the way for teardown and will have before and after shots of each component.

    Going to try the cider vinegar test tomorrow to check for magnesium, but anyone who has done repairs on one, advice/info would be awesome.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Mag content won't be much of a problem. The real issue is how much zinc is in there.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Quote Originally Posted by Rambozo View Post
    Mag content won't be much of a problem. The real issue is how much zinc is in there.
    ? Enough to be a problem, have you done one before, or is that just the type of aluminum they use?
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Trip59 View Post
    ? Enough to be a problem, have you done one before, or is that just the type of aluminum they use?
    Just from trying to weld all kinds of die cast stuff like that. Some welds great and some just vaporizes. It's all about what the alloy is, and I don't really know how to test before trying a weld. You will find out real quick if it's unweldable, so it's not like it will get messed up more than it is. If you can weld it, fine. Otherwise make the new piece, and use pins/screws plus something like Devcon aluminum or JB Weld and call it a day. Another option is to see if you can buy the part. I'm often surprised at what is available for old tools and at what price. Of course sometimes I'm surprised at how high the price is, but often by how low it is. I don't think people repair much anymore, so there are lots of parts gathering dust on warehouse shelves.
    I went in to a really old Chevy dealer once for some parts, and just for laughs I asked about the dome light lens for a 1962 Chevy truck. The counterman looked it up and a few minutes later came back with a dusty faded box from the bowels of the parts room. I was shocked and happily paid the few bucks for it. So you never know...
    Long arc, short arc, heliarc and in-the-dark!

  7. #7
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Gotcha! Something tells me this would be one of the more expensive parts... it houses the right angle gears that drive the wheel, acts as a motor end-cover, etc. If it was the other end, it'd be different. I 'could' pin it or attach a guard, but I'd definitely be more proud if it was welded, and since I'm going end to end anyhow...

    Ok, so while typing I decided to check. They do have it, it's $50.44 and in-stock. I'd still rather weld it or it'll sit on the shelf till I have an extra $50 (might be a while)

    Short of the field and a couple woodruff keys and the rubber piece the cord goes through by the handle, they have every other part for it available, so anything else I can't fix, I can order in.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  8. #8

    Default

    I see quite a few porta band saws on eBay for parts, find one with a shot motor and your set.

    Sent from my Nexus 7 using Tapatalk 2
    Don

    MTS 200 workhorse
    PowerTig 250EX <---sweet
    80 amp HF inverter arc welder
    Lincoln Buzzbox
    Rotobrute AC-35 Mag Drill
    Milwaukee mag drill
    HF Heavy Duty 16 Speed Bench Drill Press (Custom made Adjustable Height stand)

    I gotta find more junk to sell on EBaY ... Must Buy a Plasma Cutter and a Mig Welder


    Fullerton, Ca
    USA

  9. #9
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Well, for the cost of a worn out one I could buy the pieces... There's the broken out corner, a break by the guard on the other end, and the piece the idler wheel/guard bolts to has a crack on the end and around the tensioner handle.

    The good news, I lit up on the edge of the broken out corner after nothing more than a quick sandblast (no cleaning) and it puddled GREAT, like almost as nice as a piece of bar stock from the store. I'm fully confident it'll weld up fine now. I'll probably set it up for the contest (proper heading) etc. even though I have one for the category (they can choose which to count )

    On another note, brother's old lady went down trying to learn to ride, several weld repairs came my way from that. He's also my electrician, so now he's fully committed to rewiring my shop next weekend
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  10. #10
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Glad to hear it was nice weldable material. Older tools usually did use nicer metals. But man has that thing been beat up.
    Long arc, short arc, heliarc and in-the-dark!

  11. #11
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Quote Originally Posted by Rambozo View Post
    Glad to hear it was nice weldable material. Older tools usually did use nicer metals. But man has that thing been beat up.
    Yup, but it's old enough to be quality built, everything looks serviceable with a little TLC and a few repairs.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

Similar Threads

  1. Free portaband blade
    By Rambozo in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 6
    Last Post: 06-13-2014, 12:37 PM
  2. Replies: 7
    Last Post: 07-31-2013, 01:16 AM
  3. K frame stand
    By 67cudafb in forum Other Custom Fabrications
    Replies: 2
    Last Post: 03-29-2012, 02:27 PM
  4. Frame for stained glass (frame made ​​of brass)
    By donor76 in forum Hobyist Projects
    Replies: 5
    Last Post: 01-06-2012, 12:58 PM
  5. Best material for a welding table?
    By Nikola Tesla in forum General Welding Questions
    Replies: 24
    Last Post: 05-23-2011, 08:05 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •