Share
Results 1 to 8 of 8

Thread: PP205 just popped

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default PP205 just popped

    I was cutting some 5/8" steel plate and the unit popped and smoked.

    I called into the warranty/support line and left a message. I also tried to send an email to make sure this issue was seen as well as heard. But, for whatever reason my email to support@everlastwelders.com will not go through?

    I understand you guys are most likely busy and that I should be patient and wait for a phone call, but it would make me feel better to have some written correspondence. Sometimes voice messages fall through the cracks.

    I got as far as taking the case/cover off of the unit and I can see that a board is fried. I have pictures I can send someone if that will help speed things along at all. Not trying to be a PITA just want to get this going.
    2013 PP205

  2. #2

    Default

    Quote Originally Posted by Sandaholic View Post
    I was cutting some 5/8" steel plate and the unit popped and smoked.

    I called into the warranty/support line and left a message. I also tried to send an email to make sure this issue was seen as well as heard. But, for whatever reason my email to support@everlastwelders.com will not go through?

    I understand you guys are most likely busy and that I should be patient and wait for a phone call, but it would make me feel better to have some written correspondence. Sometimes voice messages fall through the cracks.

    I got as far as taking the case/cover off of the unit and I can see that a board is fried. I have pictures I can send someone if that will help speed things along at all. Not trying to be a PITA just want to get this going.


    please email RAY at tech@everlastwelders.com
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  3. #3

    Default

    Email sent. Thanks
    2013 PP205

  4. #4

    Default

    Quote Originally Posted by Sandaholic View Post
    I was cutting some 5/8" steel plate and the unit popped and smoked.

    I called into the warranty/support line and left a message. I also tried to send an email to make sure this issue was seen as well as heard. But, for whatever reason my email to support@everlastwelders.com will not go through?

    I understand you guys are most likely busy and that I should be patient and wait for a phone call, but it would make me feel better to have some written correspondence. Sometimes voice messages fall through the cracks.

    I got as far as taking the case/cover off of the unit and I can see that a board is fried. I have pictures I can send someone if that will help speed things along at all. Not trying to be a PITA just want to get this going.
    This email address "support@everlastwelders.com" has had problems for some time. Sorry about that, I did not get the email.. I changes the signature to the EMAIL I have been using for support. Hope Oleg can fix it.

    Mike R
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    Just got off the phone with Ray. He said he didn't recieve my emails. One describing the problem and one with pictures. I don't claim to be in the welder repair business, but soldering a few wires should not be a huge issue. He asked me some questions that I kind of understood. He told me that the problem could go beyond just the IGBT board, but he could send me a new one.

    I was unaware that the turn around time on a repair was a few weeks! Feeling the beginnings of regret here. I'm hoping that the problem just stems from running too long near the limit of the machines capabilities.

    My question now is if I'm sent a new board and for whatever reason the issue is not resolved will I still be able to send this thing in without any problems? Will Everlast still pick up the shipping tab?

    Also I received an auto-reply message from Everlast about my emails. Is there just a delay in the system, or did they go to the wrong person?
    2013 PP205

  6. #6

    Default

    Quote Originally Posted by Sandaholic View Post
    Just got off the phone with Ray. He said he didn't recieve my emails. One describing the problem and one with pictures. I don't claim to be in the welder repair business, but soldering a few wires should not be a huge issue. He asked me some questions that I kind of understood. He told me that the problem could go beyond just the IGBT board, but he could send me a new one.

    I was unaware that the turn around time on a repair was a few weeks! Feeling the beginnings of regret here. I'm hoping that the problem just stems from running too long near the limit of the machines capabilities.

    My question now is if I'm sent a new board and for whatever reason the issue is not resolved will I still be able to send this thing in without any problems? Will Everlast still pick up the shipping tab?

    Also I received an auto-reply message from Everlast about my emails. Is there just a delay in the system, or did they go to the wrong person?

    If Ray can send you part and you can install it then we can cover shipping
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  7. #7

    Default

    When you emailed Ray what email did you use that he did not receive it?
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  8. #8

    Default

    Oleg you have a PM.
    2013 PP205

Similar Threads

  1. PP205 problems--
    By JBnID in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 0
    Last Post: 08-23-2014, 06:21 PM
  2. PP205 my first machine!
    By Sandaholic in forum Introduce Yourself
    Replies: 6
    Last Post: 11-24-2012, 08:28 PM
  3. plasma cut pp205
    By jimmy in forum General Welder Questions
    Replies: 1
    Last Post: 11-14-2012, 04:52 AM
  4. Recieved my updated PP205
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)