  1. Default Wintertime Contest Video Review #1 - Agent4573

    So here's my first video review for entry into the Wintertime Contest. Its not my best video work, but it should do. Bought a used Powertig 185 off the forums a few weeks ago. The video shows my first TIG welds in 8 years, and they need some practice.

    Highlights of my review of the :

    Pro's:
    Torch switch is so light you don't realize you're holding it once you get the arch going.
    HF starts work awesome and rock.
    The arch is really stable and the machine is super simple to setup.

    Con's:
    Torch switch is so light I've flashed myself a few times just trying to readjust my hand.
    Pedal controls 0-185 amps all the time. It would be nice if it controlled 0-"panel setting" so you can have fine adjustment in your welding range.
    Online manual says max recommended thickness is 1/4", but I would only recommend that with preheating and possibly a helium mix for extra penetration.

    Anyway, feel free to comment on the messy garage and other suggestions.


    Poewr I-Mig 205P
    Powertig 185

  2. #2

    Default

    For some reason weld looks a little cold compared to the results i had with the 185, I did not have any problems on 1/2" x 2" cold rolled flat with no preheat. Here is a picture of a flange bending tool i made just before you purchased my welder. This was used on 240 volts 160 amps 15 cfm or 7 lpm, WP 17 torch 3/32 ER70S2 filler
    Just wondering if you are operating on 110 volts ??.
    Click image for larger version. 

Name:	Tool 1.jpg 
Views:	461 
Size:	145.4 KB 
ID:	8871
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  3. Default

    Thats on 240 Volts. I think its more technique than anything. They started to get better as I went, but another 20-30 amps would have really helped stick em together.
    Poewr I-Mig 205P
    Powertig 185

  4. #4
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    Looks like you need to slow down some and also move the torch some to direct your heat towards the toes of the weld, but not a bad start.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  5. #5
    Join Date
    Jun 2012
    Location
    Hutchinson Kansas
    Posts
    17

    Default

    It does not appear that the argon bottle is tied to anything. If it is free standing and tips over knocking the valve off you will have a high powered rocket.
    First thing to do if the bottle is not tied off is to chain it to the wall or chain it in place on a welding cart.

  6. Default

    Quote Originally Posted by bnun12 View Post
    It does not appear that the argon bottle is tied to anything. If it is free standing and tips over knocking the valve off you will have a high powered rocket.
    First thing to do if the bottle is not tied off is to chain it to the wall or chain it in place on a welding cart.
    I've cleaned the garage up and am goign to re-arrange it this week. The wooden shelves are bolted to the wall and I'm going to screw the argon tank to the side of the wooden shelves with some chain this weekend. Eventually I'm going to build a little metal table in that corner to have a nice spot to weld.
    Poewr I-Mig 205P
    Powertig 185

Similar Threads

  1. Video review of PowerArc 160 STH TIG
    By youngnstudly in forum Customer Testimonials
    Replies: 14
    Last Post: 07-09-2014, 07:02 AM
  2. winter time contest Q: does this count as a video for the contest?
    By Spike in forum Everlast Announcements, Contests and Promotions
    Replies: 3
    Last Post: 01-21-2013, 04:16 PM
  3. video review of the 200DX
    By Winky in forum Customer Testimonials
    Replies: 27
    Last Post: 10-03-2012, 12:58 PM
  4. Everlast 160 STH Video Review
    By jp2code in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 07-03-2012, 09:04 PM
  5. Everlast 210 ext Review Video
    By jp2code in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 06-13-2012, 07:25 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •