  1. #1

    Default

    7018 AC will burn fine on DC the pics posted of stick welding with the 200DX was with some old 7018 AC rod i had.

    Bottle fill price does vary depending on where you exchange, If i exchange my bottle here at the local farm store it is approx $51.00 w/sales tax for a 122 cu ft argon. If i drive 38 miles to North Kansas City it is $28.80 w/tax
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  2. #2

    Default

    Bottle price does vary by location adn also supplier. I currently get my gas from Matheson Tri-gas and pay $30 for a 330 cf bottle. I was paying close to $50 when I was getting it from Airgas.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •