Ac balance still confuses me a bit. Since different brands display it differently. So I have my ac balance set at 35% but is that 35% DCEP or DCEN?? My beads have the stacked dime look but are actually extremely smooth and I didn't know if that was because I need more amps, or maybe more DCEN. Maybe its because I'm using 3/32 tungsten and only have 1/16 aluminum fill rod left. I'm starting to think my fill rod is just too small for the welds I'm doing. Maybe with 3/32 or 1/8 fill rod I would get more definition I. My ridges...
Also DCEP gives more cleaning while DCEN gives more penetration right?
Sent from my SAMSUNG-SGH-T989 using Tapatalk 2