Share
Results 1 to 9 of 9

Thread: Project # 2 By CBMKR Decorative metal Art, Branding Iron

  1. #1

    Default Project # 2 By CBMKR Decorative metal Art, Branding Iron

    Thought this would be a good project for the contest.
    These are getting popular i made one and took it to my Daughter In Laws father in Germany and now his brother wants one.
    The letters are U for Udo ,M for Martina and C for Chenoa . The are all big in Country Western and Cowboy Stuff. Used some 3/8" x 1 1/4" cold rolled bar to bend up all the letters on the anvil or my home made pin roll. The U and the C were easy but the M always takes some time if you make it in one piece. Used some 3/8" x 1 1/4 and 3/8" x 3/4" bar for the backer plate ,I added a nut on the back to have a temporary handle to use it here, i doubt if it will ever be heated up red again but you never know. Setup the 200DX on 160 amps 8 CF 7 cup with a gas lens and welded it all up. Did a test burn to make sure all the letters were close to even and then added there sign to our sign post.

    Click image for larger version. 

Name:	Branding iron 3.jpg 
Views:	906 
Size:	138.9 KB 
ID:	8818Click image for larger version. 

Name:	Branding iron 4.jpg 
Views:	880 
Size:	140.2 KB 
ID:	8812Click image for larger version. 

Name:	Branding iron 6.jpg 
Views:	858 
Size:	144.3 KB 
ID:	8813
    Last edited by cbmkr; 12-13-2012 at 09:46 PM.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  2. #2

    Default

    Had to break this up the pic loader and the inter web we not getting along.
    Click image for larger version. 

Name:	Branding iron 5.jpg 
Views:	871 
Size:	140.5 KB 
ID:	8814Click image for larger version. 

Name:	Branding iron 2.jpg 
Views:	883 
Size:	140.6 KB 
ID:	8815Click image for larger version. 

Name:	Branding iron 7.jpg 
Views:	933 
Size:	137.0 KB 
ID:	8816Click image for larger version. 

Name:	Branding iron 1.jpg 
Views:	977 
Size:	152.6 KB 
ID:	8817
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  3. #3

    Default

    that's pretty neat. Can't beat custom crafted gifts for the holidays.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  4. Default

    Nice project, I would hate to be on the other end of that iron. Moooooooo! If cows can only talk.


    I wonder how your older 185 would have faired tigging those part compared to your new 200DX?

  5. Default

    That is a neat project! I love custom/homemade art. Definitely gives a home a more unique touch!

  6. #6

    Default

    The 185 did fine on 1/2" cold rolled to 3/4" cold rolled round , had no problem with heat and i never turned it all the way up.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  7. Default

    What kind of wood is that? Does a certain work better than others?
    I am new to welding art but I hope to share my metal art sculptures with everyone soon.

  8. #8

    Default

    The wood is Cypress it will weather outside forever, Used it for years in the wood shop making sash jamb and trim parts for older home restoration.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  9. Default

    That's pretty cool, gonna have to try my hand at that.

    Glenn

Similar Threads

  1. Replies: 31
    Last Post: 10-25-2013, 05:27 AM
  2. Replies: 3
    Last Post: 02-19-2013, 07:45 PM
  3. Project 5 by cbmkr: Gas Welding Aluminum
    By cbmkr in forum General Welding Questions
    Replies: 5
    Last Post: 10-20-2012, 11:10 PM
  4. Replies: 29
    Last Post: 09-01-2012, 05:23 PM
  5. Replies: 10
    Last Post: 08-08-2012, 11:24 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •