Thread: Project 2 from zedron. Category: Welding Cart

  1. #1

    Default Project 2 from zedron. Category: Welding Cart

    So I was at my friends shop messing around with my 200DX and he started complaining about how one of the guys who work for him forgot to turn on the water cooler and burnt up a new torch that was replaced only about 2 weeks ago. Prior to this he was complaining about how he needed a new cart for his inverter thermal arc welder too. So I said why don't you make the new cart but add a breaker to the cart that turns on the welder and cooler with a single switch. He said he doesn't have time and would love to get around to do that but time time time. So, to get some seat time in with my new welder and just general practice I offered to make one for him using his materials. The look on his face seems like he just won the lottery, lol. Its teh least I can do since I use all of his material/equipment when I need something made or fixed.

    So here we go... will be finishing either later today or tomorrow.

    Material used so far: 1/8 rectangular AL pipe, 1/8 AL plate, Misc electrical stuff, SS Rivets, SS Screws
    Filler Rod: 3/32 5356
    Tungsten: 3/32 2% thoriated
    Cup: #5
    Settings: 150A, 220Hz, 30-40% Balance, Was messing around between foot pedal and also torch switch, No pre-flow, 4 sec post flow, 18 CFH Argon flow, no pulse

    Pic 1: Completed frame. The bottom part is for the water cooler, the next part is for the welder, and the top will have a hinged top with a tray set in to hold consumables, the top will also be able to act as a little welding top. Not sure if I want to put caps on the end of the pipe or not...
    Click image for larger version. 

Name:	1.jpg 
Views:	517 
Size:	84.5 KB 
ID:	8731
    Pic 2: This is the shelf for the welder. I just drilled the holes and will just use rivets to hold it in place.
    Click image for larger version. 

Name:	2.jpg 
Views:	492 
Size:	79.1 KB 
ID:	8732
    Pic 3: Of course when you design stuff on the fly you usually come into problems. This is where I had to cut the top front support and move it back. When I put the welder in, the front brace wouldn't allow the front lid of the welder to open fully....ugh. So here it is being cut off to be relocated.
    Click image for larger version. 

Name:	3.jpg 
Views:	483 
Size:	88.2 KB 
ID:	8733
    Pic 4: Front brace cut off and welding shelf riveted in.
    Click image for larger version. 

Name:	4.jpg 
Views:	495 
Size:	92.9 KB 
ID:	8734
    Pic 5: New brace location. Since the brace is getting moved back, the tray I will insert inside will be smaller and so will the table work top, o well.
    Click image for larger version. 

Name:	5.jpg 
Views:	497 
Size:	103.6 KB 
ID:	8735
    Pic 6: Quick weld shot
    Click image for larger version. 

Name:	6.jpg 
Views:	483 
Size:	54.3 KB 
ID:	8736
    Pic 7: Another weld shot. I didn't prep the metal at all so all the oil and grease is still on there. Its not my welding cart...lol.
    Click image for larger version. 

Name:	7.jpg 
Views:	520 
Size:	64.0 KB 
ID:	8737
    Pic 8: Breaker box clamped down and drilled ready for set screws.
    Click image for larger version. 

Name:	8.jpg 
Views:	521 
Size:	92.8 KB 
ID:	8738
    Pic 9: A little green picture love. Nothing like using the Everlast machine to make a cart for a thermal.
    Click image for larger version. 

Name:	9.jpg 
Views:	529 
Size:	90.9 KB 
ID:	8739
    Pic 10: Set screws in. Dont mind my not safety foot attire...
    Click image for larger version. 

Name:	10.jpg 
Views:	470 
Size:	62.1 KB 
ID:	8740
    Last edited by zedron; 12-08-2012 at 07:55 PM.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  2. #2

    Default

    Pic 11: Went out to grab lunch and stopped at Northern Tool for some wheels. I went rummaging through the scrap he had and was able to find one piece that fit the wheel perfectly for the mounting plate. Just need to do a little trimming and we will be good to go.
    Click image for larger version. 

Name:	11.jpg 
Views:	455 
Size:	126.8 KB 
ID:	8741
    Pic 12: Other two wheels was not so lucky. Will have to do a little more cutting on these.
    Click image for larger version. 

Name:	12.jpg 
Views:	469 
Size:	92.3 KB 
ID:	8742

    So far so good. I think the design so far is good and I might copy it for when I do mine. I will modify it a little because I will need to add a part for a bottle and I will not be using a water cooler, so I can make that section some more storage with drawers hopefully. Next step is to put wheel plates on, wheels, make tray, make lid with hinges, wire up plugs, add some hooks for cables, and maybe make some type of holder for foot pedal.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  3. #3

    Default

    Pic 13: Preliminary wiring done
    Click image for larger version. 

Name:	13.jpg 
Views:	509 
Size:	95.9 KB 
ID:	8801
    Pic 14: Trays and top are in
    Click image for larger version. 

Name:	14.jpg 
Views:	515 
Size:	99.9 KB 
ID:	8802
    Pic 15: Work top complete.
    Click image for larger version. 

Name:	15.jpg 
Views:	478 
Size:	48.5 KB 
ID:	8803

    All that is left is a holder for foot pedal, add wheels, snug everything in, and then make some cord holders.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  4. #4

    Default

    Nice work. Are you using the breaker as the switch? I haven't seen the done before but I like it.

    Sent from my PC36100 using Tapatalk 2
    Just a new guy that wants to make stuff.

    PowerPro 256

  5. #5

    Default

    Quote Originally Posted by greygizmo View Post
    Nice work. Are you using the breaker as the switch? I haven't seen the done before but I like it.

    Sent from my PC36100 using Tapatalk 2
    Sure am. The breaker will act as the switch while the cooler and welder will remain in the ON position on their own switches. My friend has had a few torches burned up because the people who work for him have forgot to turn on the cooler.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  6. #6
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    Nice aluminum cart. When I get the 255 EXT I will make a cart that I never built for the 250 EXT. I may need to look into an aluminum cart. How much did the material cost for the build?
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  7. #7

    Default

    Quote Originally Posted by DVA View Post
    Nice aluminum cart. When I get the 255 EXT I will make a cart that I never built for the 250 EXT. I may need to look into an aluminum cart. How much did the material cost for the build?
    So far the wheels cost $60. As far as the AL rectangular tube goes I am not sure as it was already available in stock in the shop. I am curious though as I will be making my personal one out of AL as well. I will find out how much a stick of the rectangular tube costs and let you know.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  8. #8

    Default

    Pic 16: Complete
    Click image for larger version. 

Name:	16.jpg 
Views:	512 
Size:	106.4 KB 
ID:	8985
    Pic 17: Complete with trays having a purpose.
    Click image for larger version. 

Name:	17.jpg 
Views:	480 
Size:	76.6 KB 
ID:	8986

    I was gonna make a little holder thing for the pedal but decided not to for the time being. I dont think I will ever make one for it as this machine always has a switch on it anyways.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  9. #9

    Default

    Quote Originally Posted by DVA View Post
    Nice aluminum cart. When I get the 255 EXT I will make a cart that I never built for the 250 EXT. I may need to look into an aluminum cart. How much did the material cost for the build?
    The retail price for a 25ish foot piece of that rectangular tube is roughly $50 or so.
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  10. #10
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I like the cover on the trays. Keeps all the crud from accumulating in them, yet easy to fish things out.
    Long arc, short arc, heliarc and in-the-dark!

  11. Default

    Nice job. I like the Circuit breaker Ideal. I invision the top being used as a mini welding table lol.

  12. #12

    Default

    Thats an interesting design. I purchased aluminum to build 2 carts and the tubes is not what draws up the price. The expensive part is the aluminum sheets to make the shelfs/sides.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  13. #13

    Default

    Did a little more work. Added a handle and started to make some gizmo to hold the welder down in place.
    Click image for larger version. 

Name:	18.jpg 
Views:	456 
Size:	97.6 KB 
ID:	9026
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

  14. #14

    Default

    Bored on a Sunday so finished welder holding gizmo and painted with some leftover Black hammered rustoleum paint..... Not bad.
    Click image for larger version. 

Name:	19.jpg 
Views:	464 
Size:	73.2 KB 
ID:	9027
    Click image for larger version. 

Name:	20.jpg 
Views:	454 
Size:	53.0 KB 
ID:	9028
    2013 PT-200DX
    Ryobi Drill Press
    8" Shear
    6" Bench Grinder
    4x8 CNC Plasma Table

Similar Threads

  1. Project 2 from Trip. Category: Welding Cart
    By Trip59 in forum Other Custom Fabrications
    Replies: 1
    Last Post: 03-10-2013, 01:55 AM
  2. Project 1 from Undercut. Category: Welding Cart
    By undercut in forum Hobyist Projects
    Replies: 12
    Last Post: 01-16-2013, 05:24 AM
  3. Project 1 from ShaneJackson. Category: Welding Cart
    By ShaneJackson in forum Other Custom Fabrications
    Replies: 27
    Last Post: 10-12-2012, 02:35 PM
  4. Project 1 from CGCINC. Category: MIG Welding Cart
    By CGCINC in forum Hobyist Projects
    Replies: 28
    Last Post: 04-12-2012, 08:21 PM
  5. Project 1 Dyethor, Category; Welding cart.
    By dyethor in forum Other Custom Fabrications
    Replies: 1
    Last Post: 03-16-2012, 03:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •