Thread: Brass And Copper Belt Buckles Project 1

  1. #1

    Default Brass And Copper Belt Buckles Project 1

    Time has been in short supply this summer but had a little time to make some buckles for some friends in Germany.

    Used some .064 Brass sheet and some 1/4" solid copper grounding wire. Rough cut them out with the Supercut 50P and finished the edges on the belt sander.

    Got the too the anvil and made a dish form to the stock by working them on the anvil in a circular motion working from the center out, this will round the edges up and dish the buckle. The dimples on the front are from the wear spot in the anvil giving the etched look. Used some silver solder to attach the letters made from copper ground wire that was flattened. Also used some1/8" brass tig rod on the back for hook and the belt bar.

    tried a couple of different finishes but the marbled look from soldering and heating the copper looked best. Added some flat clear coat after cleaning and they are in the suitcase of to Germany.
    Click image for larger version. 

Name:	Brass Buckles.jpg 
Views:	2385 
Size:	147.4 KB 
ID:	10596
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Very nice, that dimpling effect from the anvil gives a lot of character. You mentioned these are already packed, but do you have a shot of the back, showing the hook and belt bar? Curious to see how they're attached.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3

    Default

    Here is a pic of a back, I have made these for years and found out that to much silver solder is not an option it is required.
    Click image for larger version. 

Name:	buckle back.jpg 
Views:	940 
Size:	148.4 KB 
ID:	10599
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  4. #4

    Default

    Thanks for posting........... very cool stuff!
    imig 200
    PowerTig 210 EXT

  5. Default

    Nice work. They look like you aged them a hundred years.

  6. #6
    Join Date
    Oct 2011
    Location
    Litchfield Park, AZ
    Posts
    370

    Default

    Belt buckles are awesome projects. I know some pipe welders and it seams like some of them spend more time making belt buckles than welding pipe.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  7. #7

    Default

    Here is one of the first ones i made back in the early 70's, all copper theme was sunrise over the mountains.

    Click image for larger version. 

Name:	old buckle.jpg 
Views:	889 
Size:	92.6 KB 
ID:	10606
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  8. #8

    Default

    So are the designs cut into the buckles rather than welded on?
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  9. #9

    Default

    The designs are made separate and welded on in thin sheets or pieces. The three i made went to Germany with me a couple of weeks ago , The country western style is big there like it was here in the 80's. Several friends there want a custom design , i will see what i can do for them this winter when i have some time.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  10. #10

    Default

    I really like the finish you were able to put on them too. That etched look is fantastic!

  11. #11

    Default

    Quote Originally Posted by cbmkr View Post
    The designs are made separate and welded on in thin sheets or pieces. The three i made went to Germany with me a couple of weeks ago , The country western style is big there like it was here in the 80's. Several friends there want a custom design , i will see what i can do for them this winter when i have some time.
    Nice, you have done a good job with the welds.
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

Similar Threads

  1. Project From EmptyNester - Belt "guide" for hovercraft
    By EmptyNester in forum Off Road Fabrication
    Replies: 5
    Last Post: 10-10-2012, 04:01 AM
  2. Welding copper and copper alloys
    By Cippee in forum TIG Welding (GTAW/GTAW-P)
    Replies: 21
    Last Post: 02-23-2012, 02:50 AM
  3. TIG brazing Brass to Steel.....?
    By CGCINC in forum General Welding Questions
    Replies: 3
    Last Post: 12-12-2011, 02:17 PM
  4. Replica naval cannon and nautical belt buckle
    By jtybt in forum Hobyist Projects
    Replies: 14
    Last Post: 06-21-2011, 10:15 AM
  5. shop made serpentine belt tool
    By Metal Wolf in forum Other Custom Fabrications
    Replies: 10
    Last Post: 03-13-2011, 12:04 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •