    Quote Originally Posted by bubbas55 View Post
    i have heard several opinions... does the argon need an air dryer....

    I do not use an air dryer for my argon and no issues here. If you need an air dryer, I would go with a different vendor because there should be no moisture in the tank.
    Miller 252
    PowerTig 250 EXT
    Evolution Rage 2
    48X6 inch Belt Sander w/ 9 inch Disk Sander
    ...

  2. #2

    Default

    Quote Originally Posted by DVA View Post
    I do not use an air dryer for my argon and no issues here. If you need an air dryer, I would go with a different vendor because there should be no moisture in the tank.
    I agree. If you are getting moisture in your welding gasses its time to switch.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

Similar Threads

  1. ??Rod Dryer Idea??
    By smithkf4gyp in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 2
    Last Post: 02-18-2018, 11:55 PM
  2. Argon Dryer
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 8
    Last Post: 11-28-2012, 02:07 PM
  3. Air Dryer?
    By Slartybartfa in forum Everlast Plasma Cutters (PAC)
    Replies: 39
    Last Post: 06-06-2012, 08:41 PM
  4. ARGON and ARGON/CO2 TANK SIZES
    By everlastsupport in forum Technical Bulletins and Tips
    Replies: 47
    Last Post: 10-13-2011, 05:19 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •