You're quick with the camera- looks like a curl of smoke in the last photo. How did you clean and prep? What kind of vehicle is the engine out of?
If you don't mind me suggesting, I notice you're entered in the current contest... you should set this kind of post up in the right format as an extra entry to the contest!
DaveO
Oxweld oxy acet gear
IMIG 200
PowerTIG 210 EXT... Amazing!
Wow, that is a hell of a hole to repair. I've seen brazing done to holes like that, but I don't think I have ever seen something like that tig welded. From the pics it doesn't look like it, but did you preheat at all?
Everlast 200DX
Everlast PT185
Shoptask 3-in-1 (not currently in my garage, but I own it...)
Any day on a motorcycle like this that ends just needing parts and labor is a good day.
4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile
Amazing!! I've had success stick welding an exhaust manifole while it was still on the truck using 7018, and just "stirring" the puddle. I believe it was a 1 in a million shot, but there was no collaetral damage, and the weld held for YEARS, until the truck was sold (1974 Ford LNT880 dump truck with a 477 gasser). I'd like to know the setup there preheat, electrode, dc or ac, etc. Looks like a beautiful repair. Jody mentioned something about using brass rod and AC TIG, But this looks like the ticket here.
"It's not magic it's experimental, kind of like washing your hands after pooping used to be." -House
Everlast PowerTig 250EX-arrived 1-26-2012
Everlast PowerCool W300-arrived 1-26-2012
Everlast PowerTig 185 Micro-arrived 1-26-2012
Everlast PowerPlasma 70-arrived 1-26-2012
ESAB MigMaster 250-borrowed
HyperTherm 151 AKA "The Light Sabre"
Linde UCC-305-964 lb. of old time water cooled TIG love-SOLD-Bad MOJO
Purox OXY/ACETYLENE
What kind of engine was it that it was rare enough to warrant this type of repair instead of just replacing the block?
Brad George
George's Welding & Repair
Amateur at TIG, MIG, and General Fabrication.
Current Equipment
AIRCO Heliwelder IV 300Amp Model - Total Awesomeness!
Hobart Handler 120v MIG
Well, it's a deep skirt block, but doesn't look like a mopar, maybe a Ford FE series or similar? S/F....Ken M
Lincoln Power MIG 300
Everlast 160STH
Miller 225 Thunderbolt (sold it)
Lincoln Squarewave 175 TIG(traded it for)
Miller DEL 200 welder/genset
Thermal Dynamics 1250XL plasma cutter
Miller XMT300
My final answer is gonna be a Merc Cruiser.
2013 PT-200DX
Ryobi Drill Press
8" Shear
6" Bench Grinder
4x8 CNC Plasma Table
Nice repair. It sounds and looks like a low expansion, high nickel content rod. Any nickel-iron allloy where the nickel reaches or exceeds mid 30's %, the low expansion "magic" starts to happen: http://en.wikipedia.org/wiki/Invar
I've had good results with it as well (a 55% nickel / 45% iron stick electrode, with the flux knocked off, and applied via TIG), but sometimes the cast iron can get a little cruddy. Interested in hearing how you prepped the cast iron because you got a nice result.
Did you weld both sides one pass each (2 passes total)? Or try to it is in 1 pass? Did you manage 1 continuous weld bead or did you beak it up? Did you skip around or "stitch weld"?
'13 Everlast 255EXT
'07 Everlast Super200P
I would be surprised if the iron doesn't crack right next to the weld once it gets back in operation.
Well it has been a few years now and it is still not leaking the motor is working just fine so far. I have done a Ford Powerstroke 7.3L and it was on a work truck and is still working over 5 years now, it cracked from water freezing in the block winter came to fast and they forgot to put the antifreeze in it, it had a hose leak so they just keep putting water in it.
Last edited by Kempy; 10-23-2013 at 01:15 PM. Reason: ADD
Everlast PowerTig 325EXT (Canada)
Everlast Power I Mig 250 (Canada)
Everlast PowerPlasma 80S (Canada)
Everlast PowerCool W300 (Canada)
Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
Miller Dynasty 400 wireless(Canada)
Millermatic 252 plus 30A Spoolgun(Canada)
OK, then I am wrong. You must be doing something right That others have not. I have seen many block repairs that have not held very long. I would not weld
blocks because it just is not worth it for someone to put all the work into the engine then have it leak again where it is welded. It may work 9 times out of 10 but one customer with a failure would cost me much more than I would make on welding blocks. I guess if it was mine I might try it, depending on how much work it would be if it did happen to fail.
I have never heard of cronatron before. I just went to there web site. Wow are the expensive. I thought Eutectic was expensive . 50 lbs of E7018 for over $300. Your cast tig rod is over $350 for 2 lbs. I find it hard to believe they have something worth that kind of expense that can not be purchased from someone else for less. I would say they just repackage and resell and not make any of there own products.
Last edited by TheGary; 10-23-2013 at 04:57 PM.
Everlast PowerTig 325EXT (Canada)
Everlast Power I Mig 250 (Canada)
Everlast PowerPlasma 80S (Canada)
Everlast PowerCool W300 (Canada)
Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
Miller Dynasty 400 wireless(Canada)
Millermatic 252 plus 30A Spoolgun(Canada)