    I was playing around with my PP205 doing some stick and realized I had left the pulse feature on from TIG. When doing stick it still was pulsing and just wondering if there is any advantage of pulsing with stick.

    I'm not sure if it would mess with the way the flux is transferred onto the weld pool but I can how it could possibly help with controlling heat. Anyways, just wondering if I stumbled upon something new or if people actually use pulse in stick welding.
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  2. Default

    My question would be is it even active in stick mode?

  3. #3

    Default

    Pulsed arc,,,makes me think of an AC buzz box switching current,,,DC arc welding is better with a constant flow of current,,,melting the rod..
    Some of those lies people tell about me, are true

  4. #4

    Default

    It does stay active in pulse on my machine.
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  5. Default

    Thanks for the clarification.

  6. Default

    Quote Originally Posted by scootarida1 View Post
    I was playing around with my PP205 doing some stick and realized I had left the pulse feature on from TIG. When doing stick it still was pulsing and just wondering if there is any advantage of pulsing with stick.

    I'm not sure if it would mess with the way the flux is transferred onto the weld pool but I can how it could possibly help with controlling heat. Anyways, just wondering if I stumbled upon something new or if people actually use pulse in stick welding.
    Interesting; I'm guessing you are in DC current and it's pulsing betwen a welding current and a lower background current. If you consider the benefits of pulsing in TIG (and perhaps to a lesser degree MIG), you can then consider analogous occasions in stick welding. One place where pulsing might be beneficial is running a root run in an open root where, conventionally, you want just enough current to open up the keyhole but not so much that you lose control of it. Possibly, with the right settings and a pulse frequency around once a second, it could be possible to lay the root; the background phase would be where the puddle freezes.

    It would also be interesting to see what effect, if any, a higher pulse frequency has on arc
    characteristics. This might be one of those occasions where one should play around with it and overcome the temptation to believe if pulsing were beneficial it would be used. One the other hand, it is only because of the introduction of modern power electronics that pulsing is possible, so stick welding had to evolve without it.

    Martin

Similar Threads

  1. Excellent Pulsed TIG article
    By earla in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 08-25-2012, 02:49 AM
  2. Question about Pulsed Mig Process
    By Oxide00 in forum General Welder Questions
    Replies: 11
    Last Post: 03-20-2011, 01:23 AM
  3. practice pieces-Pulsed Tig
    By cdale2002 in forum Other Custom Fabrications
    Replies: 10
    Last Post: 07-30-2010, 01:15 PM
  4. 250P pulsed mig
    By Metalux in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 7
    Last Post: 02-22-2010, 03:55 PM
  5. Purchased 200 ACDC Pulsed
    By wallnut in forum Customer Testimonials
    Replies: 2
    Last Post: 05-01-2009, 01:54 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •