    WP20 I ordered just arrived, checked the package to make sure UPS didn't screw up it up (box end was mashed) and the torch, consumables kit is there, but there's just the DINSE, no connectors on either water line or gas. No big deal on the water lines, I need to come up with ends for a cooler or hose anyhow, but the Ar line? I thought that would be there...

    Straight handle, flex neck design. Water cooled. 15 ft. Rated: 250 Amps DC, 175 Amps AC @ 100% duty cycle.2T/4T remote switch included (finger switch). Excellent choice for areas where maneuverability and compactness is required. Plug and play for all Everlast TIG units with the 35-70 style Dinse connectors. Suitable for use with most National brands with the 35//70 Dinse style power connector. Slight modification of the standard quick connect gas connection may be required with some national brands. Water connections are quick connect for use with Everlast Water coolers. Small consumable starter kit included. Tungsten not included.

    Are they supposed to be bare ends or was something missed at the factory?
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  2. #2

    Default Torch connectors

    I do not think it comes with the gas quick connect male end as some welders do not use a quick connect. My extra torch did not have one on it either. I had one watched on Ebay that had the connectors as a set here is the item number 170902418018.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  3. #3
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    Thanks! Like I said, I really just need the Ar, the water lines I'm going to plumb in, may use quick connects, may not, don't know yet.

    I DO know that a standard WP20 handle won't fit on the euro style WP20, where the lines connect inside the body, it's too wide to fit the handle over. Perhaps the other model has the fittings staggered more?

    I did a video review on the torch for the contest and because there were some things I couldn't find when I was looking that I wanted to reference. Not sure if it'd count for the contest or if I should even post it since I took the torch handle apart.

    A bit disappointed all around, torch came in AFTER the 4 day weekend (UPS's fault, not Everlast, it sat at the damn depot Wednesday instead of loading on a truck to my house. The stock euro handle is just as big as the WP26 I was replacing, and the new one doesn't fit it.

    I had hoped to have it for this past weekend, else I'd have waited till the other style handle was in stock.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

Similar Threads

  1. Connectors
    By aland in forum Pre-sales, Sales and Shipping questions
    Replies: 27
    Last Post: 01-07-2018, 08:34 PM
  2. How many Dinse connectors are there???
    By Brian Ski in forum General Welder Questions
    Replies: 6
    Last Post: 08-25-2014, 04:53 PM
  3. Dinse connectors??
    By fernesto in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 05-02-2013, 05:59 AM
  4. PowerPro 205 connectors for new torch.
    By Ray C in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 1
    Last Post: 09-18-2012, 04:16 PM
  5. dinse connectors
    By bobwills in forum General Welder Questions
    Replies: 21
    Last Post: 12-28-2011, 03:24 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •