    So here are a few of the updates for next year.

    NEW 2013 PowerPlasma 60/60/70/80

    - Will feature the s-75 torch now, which is a blow back start, which improves comparability for add on CNC customers, but also improves overall reliability.
    - There is a new case design which will be used for all the DX/LX/EX units which is very similar to the new 255ext.



    NEW 2013 PowerTig 200DX/225LX/250EX

    - Line will get a slight "refresh" on all the larger PowerTIGs. The Panels for all the larger PowerTIGs will have a slight redesign. More to be posted later.
    - There is a new case design which will be used for all the DX/LX/EX units which is very similar to the new 255ext.




    Click image for larger version. 

Name:	DSC02642.jpg 
Views:	1837 
Size:	138.2 KB 
ID:	8561
    Last edited by performance; 11-24-2012 at 02:03 AM.
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by oleg View Post
    stay tuned ...
    tease!!!!!
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    Lol, seriously. What a tease.
    Poewr I-Mig 205P
    Powertig 185

  4. #4

    Default

    .....................................
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	DSC02645.jpg 
Views:	958 
Size:	134.1 KB 
ID:	8560  

  5. #5
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Looks like I am going to wait for the new 2013 PowerTig 250EX for the shop and put down my Hobart 250 after 26 years of rolling around the 400lbs.

  6. Default

    When are the 2013 250EXs avalable?

  7. Default

    Ok, so I am a little confused as I was told the one I just bought this week is a 2013 model?

  8. #8

    Default

    Quote Originally Posted by Odyknuck View Post
    Ok, so I am a little confused as I was told the one I just bought this week is a 2013 model?
    Odyknuck

    you did buy 2013 model , call me and i will explain more details
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  9. Default

    I tryed calling a few time? Left message on your Cell Phone?

  10. #10

    Default

    Quote Originally Posted by Odyknuck View Post
    I tryed calling a few time? Left message on your Cell Phone?
    you need to call the office
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  11. Default

    Did that too and tryed to use the directry and you just don't exist in it lol. I will PM you with my Cell Number.

  12. #12

    Default

    Ext 201 is sales/Oleg

  13. #13

    Default

    New 250ex analog


    Click image for larger version. 

Name:	meand torah.jpg 
Views:	1109 
Size:	139.9 KB 
ID:	9131
    Oleg Gladshteyn
    Phone: 650 588 8082 / 877 755 WELD
    Cell: 415 613 6664 ONLY IF YOU REALLY NEED IT
    Email: oleg@everlastwelders.com
    Website www.everlastgenerators.com

    www.linkedin.com/pub/oleg-gladshteyn/48/b08/875

  14. #14
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Oleg View Post
    New 250ex analog


    Click image for larger version. 

Name:	meand torah.jpg 
Views:	1109 
Size:	139.9 KB 
ID:	9131
    I really like the regrouping of the knobs. Moving the gas flow to it's own group away from the 4T slope controls is great. Maybe they might someday get a new knob color, as well?
    Long arc, short arc, heliarc and in-the-dark!

  15. #15

    Default

    Rambozo, glad you picked up on that...Also if you will notice, the gas control is part of both cycles, so they are separately grouped within the group. For even further clarification, have given a couple of "directions" on the panel to make SURE customers get the setup right when going from foot pedal to torch and vice versa.

  16. #16
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    I can't see all the labels, but it looks like the new layout really groups the controls in a logical way. I'm guessing the green layout is:

    START AMPS | END AMPS
    UP SLOPE | DOWN SLOPE
    PRE FLOW | POST FLOW

    So all the starts are on the left and all the ends on the right. And having the spot time switch and knob grouped together is great. Again maybe it should have a different color knob? It would be nice if the pulse switch didn't have the printing on it because it really doesn't match with the actual positions, but I understand those come preprinted from the manufacturer. In fact except for the spot timer, I think you would be better served with just all plain black switch faces for everything. Just less confusion as more as more people now know the binary 1 and 0 for on and off, as it's used on more and more things. Because on and off really don't apply to most of the switches, anyway.
    I get the feeling this new layout will cut your support calls, at least a little.
    Long arc, short arc, heliarc and in-the-dark!

  17. #17

    Default

    Rambozo,
    Those things come standard, not much we can do about it unless we spend major $$$$$$. The colors are also limited. Most factories if they have a colored knob available will make it in only 4 colors or less. They also have to match the potentiometer shafts as well. We have new knobs scheduled, but they are not in place yet. They will be updated late this year I hope.

  18. #18

    Default

    I like the new look.. Do you guys have any pictures of the new torches?
    Jason
    Everlast 255EXT - Perfection
    Everlast PowerPro 256 - UPS Demolished
    Everlast MTS200s
    12 Ton Shop Press
    DeWalt Hand Tools/ChopSaw

  19. #19
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    I thought the picture that was put up earlier showed the knobs and description better.


    Click image for larger version. 

Name:	2013 250EX.jpg 
Views:	1137 
Size:	137.8 KB 
ID:	9134
    Everlast PowerTig 325EXT (Canada)
    Everlast Power I Mig 250 (Canada)
    Everlast PowerPlasma 80S (Canada)
    Everlast PowerCool W300 (Canada)
    Everlast PowerMTS 250S Fitted with a 30A Spoolgun(Canada)
    Miller Dynasty 400 wireless(Canada)
    Millermatic 252 plus 30A Spoolgun(Canada)

  20. #20
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    That one is easier to read. Instead of having the instructions to turn down all the slope controls to use the pedal, why doesn't plugging the pedal in, disable those controls? Seems like it's a common issue for support.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. First Test on Everlast PT 2013-250EX
    By Kempy in forum TIG Welding (GTAW/GTAW-P)
    Replies: 38
    Last Post: 03-08-2013, 06:45 PM
  2. NEW 2013 Everlast PowerMIG 210 and 200 MIG / TIG DIGITAL WELDER
    By Oleg in forum Everlast Announcements, Contests and Promotions
    Replies: 14
    Last Post: 02-10-2013, 01:13 AM
  3. Happy NEW Year from Everlast. Best wishes for 2013
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 17
    Last Post: 01-03-2013, 11:28 AM
  4. Everlast 2011 line
    By performance in forum Everlast Announcements, Contests and Promotions
    Replies: 46
    Last Post: 12-06-2011, 02:51 AM
  5. Expected Line of Everlast Stick Welders
    By performance in forum Stick Welding (SMAW)
    Replies: 4
    Last Post: 08-11-2009, 09:38 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •