Share
Results 1 to 2 of 2

Thread: Project 1 From CBMKR,Custom Welded Shop Tools And Improvements

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Project 1 From CBMKR,Custom Welded Shop Tools And Improvements

    As it would be my luck is just not good when purchasing new tools or equipment, My new RJ-9000 pound bridge jack for my 4 post lift had a bad Cylinder, Over a year old never used out of warranty ,A New cylinder was $249.95 plus shipping. I found a piece of 304 stainless with the right ID and decided to replace the tube. Cut the old base off on the lathe, Turned it around and cut off the top which was threaded for the rod end. Tacked and welded it on with the Power Tig Micro 185, 125 amps, 3/32 309 stainless rod,I just about finished with honing the bore . Will weld on the base tomorrow repaint and install it.Will post more photo's when finished .

    Click image for larger version. 

Name:	Jack Cyl 2.jpg 
Views:	391 
Size:	137.2 KB 
ID:	8516Click image for larger version. 

Name:	Jack Cyl 4.jpg 
Views:	378 
Size:	136.1 KB 
ID:	8517Click image for larger version. 

Name:	Jack Cyl 5.jpg 
Views:	409 
Size:	139.3 KB 
ID:	8518Click image for larger version. 

Name:	Jack Cyl 6.jpg 
Views:	404 
Size:	145.4 KB 
ID:	8519Click image for larger version. 

Name:	Jack Cyl 7.jpg 
Views:	406 
Size:	123.2 KB 
ID:	8520
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  2. #2

    Default

    Well the cylinder is all done , Finished honing out the cylinder and added a new US Made Polypak seal, Welded the base on with the 185 tig at 165 amps w/309 3/32 rod to get good penetration into the solid base. All back together and it works just fine. Cleaned up and added a little paint.The 304 stainless is a little over kill for material but its stronger than mild steel and i had it here in the steel bin.
    Click image for larger version. 

Name:	Jack Cyl 8.jpg 
Views:	396 
Size:	140.6 KB 
ID:	8527Click image for larger version. 

Name:	Jack Cyl 9.jpg 
Views:	384 
Size:	135.3 KB 
ID:	8528
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

Similar Threads

  1. Replies: 10
    Last Post: 03-02-2013, 04:23 PM
  2. Replies: 12
    Last Post: 12-30-2012, 05:05 PM
  3. Replies: 28
    Last Post: 12-26-2012, 02:01 AM
  4. Replies: 18
    Last Post: 09-07-2012, 06:46 PM
  5. Replies: 12
    Last Post: 07-19-2012, 08:03 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •