Thread: Works great at 130-150 amp but it crackles (sputter) at around 50-75 amp

  1. #21

    Default

    Quote Originally Posted by vicrc View Post
    hehe I am such a noob I would not even think of it as a condescending remark.
    Mark will tell you people get upset sometimes (do not believe you can get bad argon). But it happens. I would make the filter or buy one, cant hurt and argon is not cheap on smaller tanks.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  2. #22
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by cbmkr View Post
    I have some new clear water filter housings, that take approx a 2.5" round 10" filter, That would make it nice and easy to build by adding a tube in the center of the housing to push the argon down so it can work thru the desiccant. i will look at one of the filter housings today to see if it will work. I have a question, does anyone know the volume by weight of the desiccant ,trying to figure out the cu ft. per pound to order some today.
    Silica gel is 680 grams per liter.

    Update: I guess there is some variation brand to brand, probably from different bead sizes. I found one that is 800 grams per liter, for 3.5mm beads
    Last edited by Rambozo; 11-21-2012 at 11:50 PM.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. 255EXT ac arc sputter
    By slzboy in forum TIG Welding (GTAW/GTAW-P)
    Replies: 23
    Last Post: 08-13-2015, 01:50 AM
  2. HF works, but Arc wont start !!!
    By tensecond408 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 15
    Last Post: 04-04-2013, 07:34 PM
  3. tapatalk on my android tablet, and the everlast forum works great!
    By Spike in forum Forum related Questions
    Replies: 1
    Last Post: 02-02-2012, 07:07 PM
  4. Replies: 1
    Last Post: 03-07-2011, 04:34 PM
  5. Smallest compressor Available that works?
    By Gary in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 08-15-2010, 06:05 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •