Share
Results 1 to 11 of 11

Thread: Welding Table @ Work

  1. #1
    Join Date
    Feb 2010
    Location
    Coopersburg, PA
    Posts
    19

    Default Welding Table @ Work

    I built this welding table the second week at my new job since they brought me in as their new and first fabricator. The frame of the table I took the idea from one of the welding project pics on Miller's site and added my own little twist with the plasma cutting grate. This picture is just after finishing up the basic welding, but I've since painted the frame, and added a few more tool holding brackets and other details. I'm waiting on a catch pan to be bent up locally which I'll put under the plasma grate and be quickly removable to empty when needed.

    The table was mig welded with my Lincoln 175 hiding behind the PowerPro205, but I did use the Everlast to cut out the 18 x 21" opening. Our 30amp breaker kept tripping from extended use at 45+ amps so I had to do short 1.5" sections and keep taking breaks.

    Specs of the table are:
    4x8', 1/2" thick top sheet
    2x2", 3/16" wall square tubing
    3" non-marking casters, overall height of 5.5" (if I recall right) with locking wheel and swivel
    total weight approximately 750-800lbs. Raw materials weighed in at 850 or so on invoice, before cutting out 18x21 plate.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	IMG955155.jpg 
Views:	914 
Size:	61.6 KB 
ID:	494  

  2. #2

    Default

    Nice job. Good looking Fab. bench.

  3. #3
    Join Date
    Feb 2010
    Location
    Coopersburg, PA
    Posts
    19

    Default

    Some other pics I took:
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	welding table almost done.jpg 
Views:	748 
Size:	47.6 KB 
ID:	499   Click image for larger version. 

Name:	welding table clamp rack.jpg 
Views:	771 
Size:	47.5 KB 
ID:	500  

  4. #4

    Default

    Quote Originally Posted by 91TSiGuy View Post
    Some other pics I took:
    Nice table, but I hate to say this as most others are too shy to say it. But why is the table installed in what is obviously a hospital operating room. That cannot be your shop, there is nothing to trip over and no pile of slag or steel on the floor.

  5. #5
    Join Date
    Feb 2010
    Location
    Coopersburg, PA
    Posts
    19

    Default

    It's a car shop, just a step above the average.

    I'm set up back where that foldable wall was in this pic.

  6. #6

    Default

    Funny Geezer. I was thinking the same thing. Just did some welding on a mud truck and I tripped all over stuff. That environment is not healthy.

    Just kidding, nice table and shop. I really like the green in the corner on the one shot.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7

    Default

    If I find the time, I post a picture of my table I built from scratch that I use. Its similar, but different.

  8. Default

    Looks more like a museum in the second pictures.How could you ever get any work done in that kind of environment.I bet if someone were to throw a gum wrapper down someone would catch it before it hit the ground.Very nice.

  9. #9

    Default

    That is a fine piece of work, thanks for taking the time to post it!
    Big Willy in Rockford, Il. Power Pro 205, Lincoln 140 Mig, Oxy/Acetylene rig with a Cobra Torch, Full up Motorcycle shop.
    http://projectoldwing.com
    wruehl@hotmail.com
    Active Ironbutt Member.

  10. #10

    Default

    my dream job! everything is clean... everything.... I hate working at a landfill!
    I'd like to think I'm the guy they are talkin about when they say, "he could F%^& up a cannon ball in a plowed field."
    .................. /...\
    ..............-...|.....|
    ...*.......-'. \..\__/
    ....\.-'.........\
    ... /......... _/
    ...|......... /"
    ...|.... /_\'
    ....\....\_/
    ......""""

  11. #11

    Default

    Its so clean and neat. I love it! I wish I had that much room in my work area.
    Everlast lx225
    Hobart Handler 210 with spool gun
    Hobart Stickmate LX
    Thermal Arc 400GMS
    40 amp Northern Tools plasma torch
    130 chicago electric tig welder
    90 amp chicago electric flux mig
    10"-22" Grizzly lathe
    15"-5.5" Grizzly vertical end mill

    In need of nice TIG machine. drooling over PowerTig 250ex

Similar Threads

  1. NOt welding related but some of my recent hat work
    By ironmanjay in forum Other Custom Fabrications
    Replies: 10
    Last Post: 06-07-2013, 10:34 AM
  2. Grounding the work table
    By CraigJ in forum General Welder Questions
    Replies: 52
    Last Post: 06-06-2012, 05:47 AM
  3. Looking for a TIG/Plasma that would work on a CNC table as well.
    By Tacoma747 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 11
    Last Post: 04-12-2012, 06:19 PM
  4. welding/ machine work I know there is a better way.
    By ScratchStart in forum Heavy Equipment and Commercial Projects
    Replies: 8
    Last Post: 04-26-2011, 02:19 PM
  5. PP256 Work table/cart
    By dirtyfarmer in forum Other Custom Fabrications
    Replies: 7
    Last Post: 06-24-2010, 11:52 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •