    100% my design, completely custom, and the first piece of furniture I have ever built. What do you think. What should I sell it for? Wonder if Everlast will trade me for a Plasma Cutter lol?


    Here are the details on this piece:

    36" square by 17" tall.
    3/4" 16 gauge steel tubing was used for the frame.
    3/16th" plate steel was used for the feet.
    1/2" reclaimed plywood was used for the upholstered inserts.
    Upholstery is a "wheat" colored faux Emu leather for easy clean up.
    Paint is a "Dark Bronze" hammer finished.
    I-MIG200 was used to weld it up. (couldn't be happier with the welder at this point. I have a very small gas leak that I need to find. But other than that I love it)

    These are the legs all welded up.


    This is the frame all welded up.


    And here it is complete and ready to be sold.

  2. #2

    Default

    Very nice. Do you weld tabs in the back and attach the panel from the inside? How is the weight with all the sq tube. Looks VERY rich though. Oleg would have to comment on the plasma cutter. He might need a couple more pieces

    I to am attached to the IMIG-200, that and a PP50 will make you lots of projects/cash for sure.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Nicely done! Any clever access points for storage?
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  4. #4

    Default

    Quote Originally Posted by DaveO View Post
    Nicely done! Any clever access points for storage?
    Thank you. Not on this one. I plan on building more though that are based on this frame but all slightly different from the next. No two will be 100% the same and access points where something I was going to attempt at some point. I'm still very limited on tools. More complex designs will require more tools. I built this with and angle grinder, drill, jig saw, an electric staple gun, a couple wrenches, and my I-MIG200.

    Thing on my to buy list are, Table saw, Plasma cutter, large shop compressor, paint gun, powder coating setup, metal band saw, metal scrolls, metal brake, Picket twister, and the coveted plasma table. Maybe even a forge and anvil too.

    lmao just a small list of things. Nothing to expensive lol.

  5. #5

    Default

    Quote Originally Posted by everlastsupport View Post
    Very nice. Do you weld tabs in the back and attach the panel from the inside? How is the weight with all the sq tube. Looks VERY rich though. Oleg would have to comment on the plasma cutter. He might need a couple more pieces

    I to am attached to the IMIG-200, that and a PP50 will make you lots of projects/cash for sure.
    I was going to weld the tabs but opted out for a few reasons. I was tired of cutting metal with an angle grinder. The plywood is only 1/2 thick so I was worried about strength. What if someone stands on it and it breaks? And I wanted to make those bolt heads functional. So I cut 5 more pieces of 1/2 plywood, one for the top and one for each side. These are bolted to the inside of the frame and each of the individual panels are attached to that. It's very strong.

    As far as weight... I'm not sure. I don't have a way to weigh it at the moment. Need to go buy a bathroom scale or something. If I had to guess I'd say between 50 and 70 pounds. But I'm thinking much closer to 50 pounds than 70.

  6. #6

    Default

    Well it still looks really good. Cosmetics will sell. Shipping weight will help sell it too, so 1/2" plywood and steel is something to think about in the future.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. #7

    Default

    Thank you.
    Alvarez Metal Works
    Syracuse/DeWitt, NY
    www.alvarezmetalworks.com
    www.upstate4x4.com

    *** PowerTIG 210 EXT *** PowerPlasma 50 *** I-MIG 200 ***

Similar Threads

  1. 80 on CNC table
    By RibbedGiraff in forum Everlast Plasma Cutters (PAC)
    Replies: 6
    Last Post: 02-18-2016, 06:57 PM
  2. coffee table
    By donor76 in forum Metal Art
    Replies: 64
    Last Post: 01-10-2013, 02:36 PM
  3. Surface Plate Coffee Table, Project #1, d.fisher
    By d.fisher in forum Metal Art
    Replies: 21
    Last Post: 03-14-2012, 12:53 AM
  4. Surface Plate Coffee Table, Project #1, d.fisher
    By d.fisher in forum Metal Art
    Replies: 0
    Last Post: 02-21-2012, 10:17 PM
  5. A coffee table and bathroom remodel
    By jameswswanson in forum Personal Projects (no welder required)
    Replies: 11
    Last Post: 04-21-2011, 03:39 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •