Share
Results 1 to 20 of 62

Thread: Teardrop camper build

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Default Teardrop camper build

    I started building a teardrop camper. Made lots of progress. Too bad I welded the axles on backwards and have to cut them off to re-weld them..


    Steel coming home:



    The start:





    The tongue will be retractable:



    Stabilizer jacks and axles on backwards haha!



    Wheels:



    Getting there. Lots of bracing left and small stuff.

    All welded with a 200DX. Wish I had a MIG welder right about now...
    Purple Fabricator 211i

  2. #2

    Default

    Purple Fabricator 211i

  3. #3

    Default

    Is that a torsion axle? The only one's I have used are the regular axles with leaf springs.
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  4. #4

    Default

    Quote Originally Posted by SeanMurphy265 View Post
    Is that a torsion axle? The only one's I have used are the regular axles with leaf springs.
    Yea they are torsion axles.
    Purple Fabricator 211i

  5. #5

    Default

    Are they the ones from Northern? Keep us posted on the progress and maybe rough cost. Wheels, steel, etc. Looks like a fun project.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  6. #6

    Default

    I bought the axles from eBay. As it is right now, I have around $1400 in it.


    RV Teardrop 120 Volt 15 Amp All Weather Male Receptical: $28.00
    Wheels shipped: $184.83 for 3 wheels
    3 Center caps: $25.47
    2 Stabilizer jacks: 38.94 shipped
    Axles:$260
    Vent fan: $185
    Tongue jack: $45
    Tongue hitch:$15
    Steel: $220.00
    Tires: T205/70R15 - $259.89
    Misc: $71.06


    TCI: $1333.95

    Well today was kind of productive. I ran out of argon, and paint. Plus it was kind of windy which made welding difficult because it kept blowing my shielding gas away. I would go refill my bottle and buy more paint, but I have to go to work tomorrow. So it will have to wait.

    Half of the frame is painted. Also, I have a little bit of welding to do. I tacked up the A frame, but it has to be welded all the way up. Then I have to wrap each end of the center support, because they both will act like a trailer hitch. Since the tongue will slide in/out and the rear will have a hitch receiver.

    Doesn't look like I did much, but I flipped the axles, and added another support beam, cut/fitted the A frame, and tacked most of it, welded some. Sanded and painted what I could.

    Pics:

    Front view. It's upside down too.



    Rear view:



    It will be another couple weeks before another serious update. Before I can even start working on the cabin, which will go fast, I need a few things.

    Door
    Hatch hinge
    Epoxy
    Bed liner

    and of course, wood.
    Purple Fabricator 211i

Similar Threads

  1. Still a happy camper
    By Winky in forum Customer Testimonials
    Replies: 6
    Last Post: 04-05-2014, 04:40 PM
  2. Happy camper!!
    By Jody Miller in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 12-05-2012, 01:32 PM
  3. Teardrop Trailer/M/C hauler.
    By 225 in forum Personal Projects (no welder required)
    Replies: 26
    Last Post: 05-15-2012, 01:18 AM
  4. VW Camper Van Exhaust/Muffler (jakeru's #7)
    By jakeru in forum On Road Fabrication
    Replies: 0
    Last Post: 06-23-2011, 05:42 AM
  5. Tear Drop Camper / tiny campers
    By SeanMurphy265 in forum General Welding Questions
    Replies: 7
    Last Post: 06-21-2011, 02:53 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •