Long arc, short arc, heliarc and in-the-dark!
Your filler is regular steel, from what I can see of the copper color filler in the pic and I suppose your metal is as well? It won't give the heat lines like Stainless.. Also for a shinier weld, adjust your argon flow up or use a gas lens or a smaller one.