Quote Originally Posted by johnson697 View Post
what size of cup would you have used if you was welding this rambozo?
Since I would only do short welds on stainless exhaust tubing, and move around to help control the heat put into the part, and warping, I would probably use a 1/16" tungsten and a #7 or #8 as long as I could get access with it.