  1. Default How to make gold/purple welds

    HELLO EVERYBODY IM NEW IN THE WELDING BUSSINES.. I PURCHASE A 200DX 6-7 MONTS AGO AND SLOW BY SLOW I CAN MAKE MORE JOBS IN THE SHOP...
    MY QUESTION IS HOW THE PROFESSIONAL RACE BUILDERS MAKE THE GOLD DIMES IN HIS JOBS...
    HERE IS A PIC OF A FEW JOBS I DID





    IF YOU LOOK AT MY WELDS THEY DONT LOOK SHINY

    I WOUL LIKE MY WELDS LIKE THIS



    I HOPE THE EXPERTS CAN HELP ME

    REGARDS FROM MONTERREY MX

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    If you overheat stainless it will get dark and lose the shine. Also you need to have good argon coverage whenever it's red hot. Be sure to keep your torch over the weld after you stop the arc, and you might even need trailing coverage if you weld longer runs. For an inch at a time you should be ok with just the torch. Also you will need back purge for tubing like that.
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    what size of cup would you have used if you was welding this rambozo?
    250 ex
    205 mig
    milwaukee grinder
    140e mig

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by johnson697 View Post
    what size of cup would you have used if you was welding this rambozo?
    Since I would only do short welds on stainless exhaust tubing, and move around to help control the heat put into the part, and warping, I would probably use a 1/16" tungsten and a #7 or #8 as long as I could get access with it.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5

    Default

    Your filler is regular steel, from what I can see of the copper color filler in the pic and I suppose your metal is as well? It won't give the heat lines like Stainless.. Also for a shinier weld, adjust your argon flow up or use a gas lens or a smaller one.
    Last edited by performance; 11-07-2012 at 08:32 PM.

  6. Default

    thanks for i really aprecciate the help... i will post more pics of my next stainless welds... PERFORMANCE yes is regulaicr steel.. i think is easier to get a shiny weld with the stainless steel parts/rod ...

    thanks alot

Similar Threads

  1. Hello from gold country CA
    By Gunther in forum Introduce Yourself
    Replies: 4
    Last Post: 06-20-2017, 12:28 PM
  2. Cant make up my mind
    By Steveg63 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 05-28-2014, 02:55 AM
  3. Georgia Gold
    By Titan winch in forum Other Custom Fabrications
    Replies: 3
    Last Post: 04-03-2012, 04:28 PM
  4. purple torch or S45 torch the best
    By trickbiker in forum Everlast Plasma Cutters (PAC)
    Replies: 3
    Last Post: 12-06-2011, 02:58 PM
  5. How do I make the arc quieter?
    By nanaf in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 11-05-2010, 12:12 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •