Quote Originally Posted by zoama585 View Post
The CK 130 or better yet the CK Flex-loc 130 with a superflex lead is the way to go as it will handle 150 amp ac or dc at 60% duty cycle with no problems.
If you go up to the next size torch that's gas cooled you'll have a much heavier lead that pulls on your torch and gets in the way.
Here's a couple pics of the CK 130 and CK 210 hanging to give an idea of flexability. Click image for larger version. 

Name:	IMG_1217.jpg 
Views:	527 
Size:	145.5 KB 
ID:	8407Click image for larger version. 

Name:	IMG_1215.jpg 
Views:	517 
Size:	146.5 KB 
ID:	8408 The cable/lead is much heavier on the 210.
He is dead on the money. I'm using a CK130 flex and LOVE it!