Greetings all,
I've got a PT200DX at home and am liking it so far. Liking my skill at TIG welding...well...that's another topic. I do alright but only seat time will make it improve I suppose.
My one major complaint about the machine is that big mother $%&#*@ WP26 torch and massive cable. My word, I had to introduce many more dumbell curls in my exercise routine in order to use it for any length of time.
So here's the nitty gritty of what I'm trying to figure out. Sure, I'd love to have a water cooled torch for size and comfort. But to be honest I don't weld for hours on end, weld at the peak output of the machine, nor do i want the added expense of a coller. They are quite expensive, even if you make it yourself, unless you find some KILLER deal (i.e. practically free from a scrap yard).
My thoughts are to buy a CK gas cooled torch with a flex head, superflex hose, and in the range of 125-150 amp output. Seems that the CK17 fits this role well. If I ever have the need of going above that range I can tolerate the WP26 that came with the machine for that particular job.
So I'm looking for opinions on this approach to a new torch. Does anyone do the same thing? Would it be better and less frustrating to go with a 200 amp gas cooled torch? Maybe I should go even smaller, say a CK9 or something?
Discuss...