Thread: Changing to a gas lens what do I need.

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. Default Changing to a gas lens what do I need.

    I want to try a gas lens setup.

    Using a everlast 200DX tig, whihc has the wp-26 torch I think.

    Have ordered some gas lenses and some collets to suit. I wonder though now if I also will need some "gas lens insulators" the white ceramic ones as well?

    Peter

  2. #2

    Default

    Quote Originally Posted by PeterA View Post
    I want to try a gas lens setup.

    Using a everlast 200DX tig, whihc has the wp-26 torch I think.

    Have ordered some gas lenses and some collets to suit. I wonder though now if I also will need some "gas lens insulators" the white ceramic ones as well?

    Peter
    The regular insulator should work but you will need gas lens ceramic cups, the regular ones won't work.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  3. Default

    Quote Originally Posted by zoama585 View Post
    The regular insulator should work but you will need gas lens ceramic cups, the regular ones won't work.
    Yep ordered collet and cup.

    They sent me a 1.6mm gas lens collet but I ordered a 2.4mm one. Can I just drill the hole out to suit, t looks like it should be fine.

    Also I ordered a no.7 which fits the collet body, and I ordered a no.10 lens too. But this will not fit the collet thread as it is like twice the size. What is the largest size lens I can go Up to on a wp26 torch using 2.4mm tungstens?

  4. #4
    Join Date
    Oct 2012
    Location
    Canada, Suttonwest, Ontario
    Posts
    676

    Default

    Here is a list of Parts for a WP-26 from WeldCraft.Click image for larger version. 

Name:	TIG Torches Alumina Nozzles for Gas Lens & Std. Gas Lens.jpg 
Views:	9548 
Size:	143.0 KB 
ID:	8404Click image for larger version. 

Name:	TIG Torches Gas Lens.jpg 
Views:	5670 
Size:	144.9 KB 
ID:	8405Click image for larger version. 

Name:	Weldcraft-Catalog 2012  WP-17,18,26 & CS200,300,410 .jpg 
Views:	2382 
Size:	147.5 KB 
ID:	8406

  5. #5

    Default

    Quote Originally Posted by PeterA View Post
    Yep ordered collet and cup.

    They sent me a 1.6mm gas lens collet but I ordered a 2.4mm one. Can I just drill the hole out to suit, t looks like it should be fine.

    Also I ordered a no.7 which fits the collet body, and I ordered a no.10 lens too. But this will not fit the collet thread as it is like twice the size. What is the largest size lens I can go Up to on a wp26 torch using 2.4mm tungstens?
    It's OK to drill it, I've run into the same thing. There are two sizes of cups, small and large for gas lens on the 26 torch. Small is fine for most work on steel and aluminum.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. Default

    yep drilled it out and seems okay.

    But looks like I will need a longer white ceramic insulator collar/bush thing though. There is a gap between the screwed on gas lens and the existing white insulator.

  7. #7
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by PeterA View Post
    yep drilled it out and seems okay.

    But looks like I will need a longer white ceramic insulator collar/bush thing though. There is a gap between the screwed on gas lens and the existing white insulator.
    The gas lens does not contact the insulator (Teflon BTW). Just like the standard collet body doesn't contact it either. Only the ceramic cup or nozzle hits it and presses it against the torch body. There are two sizes of gas lens insulators depending on if you have the standard gas lens or the jumbo version. Some brands have a single large insulator and others have you stack the gas lens version on top of the standard one. Also the ceramic cups are different because the thread sizes are different. The maximum size depends on the brand you use, and there are some brand to brand differences in the really big parts, so try to stick to one brand. In the small size you can go to #8 in WeldCraft, and the big one goes to #12 plus a special short jumbo that is almost an inch across. CK has some even bigger versions for titanium in their gas saver line. There are other brands that offer "champagne" cups, mostly for titanium and other reactive metals. One thing to keep in mind is that the larger the cup the more gas you will need to make it work properly. For most welding a #7 is a good general size.

    The two piece...



    And a single piece version.



    It really helps to learn the proper names for all the parts so people know what you are talking about. The metal part with the screen in it is the gas lens, they come in different sizes to fit the tungstens. The collet goes inside that to grip the tungsten and is also sized by the tungsten. The ceramic cup or nozzle screws on the front and has a number size that is the number of sixteenths of an inch the opening is, so a #7 is 7/16" and a #8 is 1/2". The insulator goes between the cup and the torch body and seals the gas, so some makers call it a cup gasket as well.

    Here is a nice diagram of the different parts.

    Last edited by Rambozo; 11-09-2012 at 09:41 AM.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Anyone using a gas lens?
    By HemiRod23 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 07-23-2012, 06:16 PM
  2. Project #3 from DVA: Stool for changing brakes
    By DVA in forum Other Custom Fabrications
    Replies: 7
    Last Post: 10-19-2011, 04:19 AM
  3. Changing gas to Mig Aluminum
    By Ram48 in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 5
    Last Post: 08-12-2011, 02:15 AM
  4. changing settings while welding
    By dgarnier in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 04-05-2011, 01:36 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •