16 ga steel settings?
Got some hood time today, got a bit confused. Cleaned the zinc off of a piece of exhaust pipe cutoff, tried to run beads around the edge. Keep in mind this is essentially the first time I've TIG'd in 13 years or so...

Top right was first, top left was second and the bottom was third. First TIG welds in earnest since I got the machine set up.
Having a bit of an issue with the filler balling. Nice clean arc, slow puddle forming, but the filler is balling and dropping before I can get it into position. Been running between 45 and 65 amps or so, on this and some 16ga square tube.
Welded up a 45 on some 3/4 square tube then propped it up with the peak up and bashed the hell out of it with a hammer. One joint bent, the others broke. OK looking beads, crappy penetration (beveled the edge half thickness, no gap) Again, filler balling up before I can get it to the edge of the puddle. Using 1/16 Lanthanated, 1/16 ER70S-2 filler
Thoughts?
Trip Bauer
Former USN HT
Everlast 200DX New Model
Hobart Handler 125 MIG
Van Norman #12
Atlas 12" engine lathe
'98 RoadKing - 84 Ironhead - 59 Ironhead