    Default Welding a zinc yellow plated grade 8 bolt

    I need to tack a zinc plated bolt to a steel plate... should I just grind off the zinc plating where the tacks will be? Also will the heat greatly affect the strength of the bolt? (Should I do 1 tack and let it cool before the next tack??)

    The bolt is a 1" x 3" bolt so it will take a lot of heat to get it hot.

    I also will be doing the same to a 1.5" bolt on the next project......
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

  2. #2

    Default

    Quote Originally Posted by ShaneJackson View Post
    I need to tack a zinc plated bolt to a steel plate... should I just grind off the zinc plating where the tacks will be? Also will the heat greatly affect the strength of the bolt? (Should I do 1 tack and let it cool before the next tack??)

    The bolt is a 1" x 3" bolt so it will take a lot of heat to get it hot.

    I also will be doing the same to a 1.5" bolt on the next project......
    If you are tack welding a 1" gr8 bolt to a plate, I doubt you need to be concerned with the strength of the bolt dropping. Is the plate intended to tranafer load from the bolt? Is grade 8 specified for some reason?

    You can grind the zinc or just weld it as is. The zinc could add a very small amount of porosity to the welds, but it is minimal. Grinding won't hurt anything.

    The proof load for a 1-8 gr8 bolt is over 72,000 lbs.
    For a 1.5-6 grade 8 is is over 168,000 lbs.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. #3

    Default

    The tacks are to keep it from spinning or falling out. The plate will be welded to a pipe. The bolt head will be inside the pipe never to be seen again....
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

  4. #4

    Default

    Your "tacks" will have to resist about 900 ft-lbs tightening torque if assembled dry.

    Assuming a standard 1-1/2" head on the bolt, your welds will be at 3/4" radius (conservative), which makes ~ 14,500 lbs shear requirement in the sum of your welds to prevent torque out.

    This all assumes that a Gr8 fastener was required and will be properly tensioned (thus the 900 ft-lb reference)

    To go another step, assuming you are using 70ksi filler, and using a 50% knockdown for shear (again, probably conservative), you have 35,000lb/in² shear strength in the material.

    14,500lb / 35,000lb/in² = .414 in² weld throat area requirement.

    If you have a .25" weld throat, .414in²/.25in = 1.65in total weld length...probably a bit more than just a few tacks.

    This is weld throat, not weld leg length and alll of this may be incorrect as I didn't check the math.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  5. #5
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    How thick is the plate? Why tack vs weld it in?
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

  6. #6

    Default

    .250 plate. When I say tack I do not mean small tacks. I mean .5in long beads on each of the sides.

    The "job" did not specify grade 8. I just went with grade 8 for the higher strength.
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

  7. #7
    Join Date
    Sep 2011
    Location
    Middleburg Florida
    Posts
    556

    Default

    I'd buzz the coating off, flatten the markings, chamfer the edges and burn it in, opposite sides sequentially.
    Trip Bauer
    Former USN HT
    Everlast 200DX New Model
    Hobart Handler 125 MIG
    Van Norman #12
    Atlas 12" engine lathe
    '98 RoadKing - 84 Ironhead - 59 Ironhead

Similar Threads

  1. Issues (Yellow) Supeer Pro 160, will not switch between modes
    By hhubred in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 2
    Last Post: 04-25-2013, 10:50 PM
  2. Parker Welding Grade 1/4" ID Hose
    By cbmkr in forum Buy, Sale or Trade
    Replies: 0
    Last Post: 08-18-2012, 03:28 PM
  3. Welding grade 2 titanium
    By welderdude in forum General Welding Questions
    Replies: 11
    Last Post: 08-09-2012, 07:50 PM
  4. Zinc coated steel?
    By posixPilot in forum General Welding Questions
    Replies: 29
    Last Post: 03-04-2012, 03:41 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •