Want to confirm the settings when using the plasma cutting feature on the Super 200P
All Dials set to Zero or Min. except for Current Control
AC/DC set to DC
2T/4T set to 2T
Pulse/DC switch to DC
Mode Switch down (Plasma Cutting)
Air At 65 - 70lbs
I am assuming the Current Control dial is the only dial used to select amperage for plasma cutting