Share
Results 1 to 7 of 7

Thread: Everlast Power I-MIG 200

  1. #1

    Default Everlast Power I-MIG 200

    So I got my welder on the 19th and decided to do a complete review/setup of the welder. Step by step from the unboxing to the first welds with it. Some of these videos are long as hell but if you're thinking about buying one of these WATCH ALL THE VIDEOS. I'm sure there are a few details in the video that will help you out.

    To some thing up: Keep in mind the saying, "you get what you pay for" is very true. I'm not saying this is a bad welder by any means. However as you will see in the videos the low cost comes with a price. Be ready to take this welder apart and make sure every nut, bolt, screw is properly snugged down. In my opinion this is not a problem for me. It's a fair trade so long as the welder lasts and does the job properly. Another issue I had was a leaky flow meter/regulator. As you will see in the videos I was able to fix this too. And the last issue I had was with packing. They put the flow meter/regulator in the box inside a not so padded UPS bag. This let it flop around in there during shipping and scratched up my case pretty good. Outside of these three thing this thing is a real nice welder so far. I've only tested it doing a few small beads but it does a great job. Tomorrow will be the start of my welding cart/welding table build. That will let me really put this thing to the test to see what it's made of. I'll be sure to report back. However at the moment I wouldn't have any problem recommending this welder to someone (I would make sure they knew the trade off that I experienced for the low cost.) I'm really happy with my purchase and did enough homework on other people's experiences with Everlast to have a pretty good idea of what to expect and look for. If you guys would address the few issues I had I think this would be a much easier sell to the skeptics. However I'm a happy customer so far.

    Anyway here are the videos.


  2. #2

    Default


  3. #3

    Default


  4. #4

    Default


  5. #5

    Default


  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Is your flowmeter calibrated in liters per minute (lpm), or cubic feet per hour (cfh)? The figures you mention are correct for CFH but I was under the impression that Everlast flowmeters are in LPM so you need to basically cut the CFH values in half.

    Nice videos. Shipping damage is unfortunately an issue with something in the weight class. Like you say, for the price difference, you can do a little of the QC yourself.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7

    Default

    You're right about the flowmeter. Wish I would have caught this before I wasted all that gas lol. Oh well live and learn.

    Just about all wrapped up with my welding cart/table that I'm building. Love the welder so far. Wish I would have made the move and bought one along time ago. Could have same myself a bunch of money.

    I'll start a new thread and post the videos of my welding cart/table when I'm finished with it tomorrow.

Similar Threads

  1. where can i buy a new tig torch for my everlast power tig 200 dx-d
    By steve1989 in forum General Welding Questions
    Replies: 4
    Last Post: 12-28-2015, 12:04 AM
  2. power rating for everlast #20 torch?
    By WhitsonMetal in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 06-10-2015, 02:03 AM
  3. New to EverLast Looking at a Power Ultra 205
    By Zaichuk in forum Introduce Yourself
    Replies: 1
    Last Post: 03-28-2011, 12:56 AM
  4. Everlast Power Ultra 205 plasma cut
    By worntorn in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 3
    Last Post: 06-17-2010, 03:59 PM
  5. Everlast Power Plasma 50 in Canada
    By everlastsupport in forum Customer Testimonials
    Replies: 2
    Last Post: 10-05-2009, 01:07 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •