    I have a Powertig 250EX for almost two years and love it. I Have noticed that the gas line does not hold the gas as my other machines do. The argon leaks down in the line after closing the valve on the tank. Takes about 5 minutes to leak down to nothing. My Hobart Handler 210 mig machine holds the gas fine for almost ever.

    Is it normal for the Powertig 250EX to leak down like that?

    BTW...if you ever get a chance, open up your machine and look inside. (Make sure you unplug it first and ground it so any contact to electrical parts is not met with a zap!)

    It is amazing the engineering that went into it. Lots of heavy duty parts. I did notice when I opened mine up that the electrical connection to the torch was really loose. Tightened it up and it runs a whole lot smoother.
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

  2. #2

    Default

    Soap all your connections... Not sure what pressure the Argon is set after the fixed regulator and goes through the flow meter but seems pretty high. (50-80 psi?? Guessing) I have found the screw clamps were not sealing the hoses really well to the barbed fittings. My 200dx was doing the same until I tightened them down a couple times.
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  3. #3

    Default

    Always bleed down the gas in the lines when you are done welding, before turning off the machine. Also let the machine run a bit to cool as well. The pressure on the gauge/regulator diaphragm and unit/torch hoses puts extra wear on them and will shorten their life.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4

    Default

    Quote Originally Posted by everlastsupport View Post
    Always bleed down the gas in the lines when you are done welding, before turning off the machine. Also let the machine run a bit to cool as well. The pressure on the gauge/regulator diaphragm and unit/torch hoses puts extra wear on them and will shorten their life.
    Well then maybe having a slight leak that gets rid of the pressure is good? It leaks down in about 5 minutes and is not really a problem it's just that I find it interesting that my Hobart does not leak down. I shut off all my gas when done welding anyways so it is not like I lose a lot of gas.
    Powertig 250EX
    Powerplasma 50
    Hobart Handler 210 with spoolgun
    Cobra 2000 / Henrob O/A torch
    Drill press / metal brake / 36 ton air hydraulic press
    Franzinated modified Craftsman 33 compressor
    Lots of other metal working tools

Similar Threads

  1. New 160STH gas leak?
    By tomm in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 04-22-2018, 03:21 PM
  2. Argon leak inside My new Everylast 205S
    By bcstexas in forum General Welder Questions
    Replies: 4
    Last Post: 11-27-2013, 09:24 PM
  3. Project 1 from Jason: Windshield Leak Fix.
    By Jason in forum Welding Repairs
    Replies: 2
    Last Post: 06-02-2011, 05:05 AM
  4. Argon regulator leak
    By robsthomson in forum TIG Welding (GTAW/GTAW-P)
    Replies: 29
    Last Post: 01-15-2011, 07:21 PM
  5. Threaded fittings leak solver!
    By dwdw in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 01-14-2011, 12:47 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •