Share
Results 1 to 11 of 11

Thread: Speeding up the rust process?

  1. #1

    Default Speeding up the rust process?

    I'm working on a project and I need to speed up the rust process.
    My thought was some type of acid but I want to make sure it looks natural and not weird.

    Any chemists out there? Any ideas?
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default

    Bring it to PA and sit it outside...it will rust fast...

    Might try some salt on it, but it isn't going to look natural in any short time. Oxalic Acid might work as well. It would still take a fair amount of time. Pretty much any quick method will probably either look too even o won;t be "deep" enough to look real once you wash off all of the deposits form teh chemicals (like salt).
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. #3

    Default

    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  4. #4

    Default

    Thanks for the links!

    I making a metal art "rat rod" and I want it to look either rusty all over or, paint it, then sand down the paint so the metal shines through in spots and then make those spots rust. My actually be better off just letting it sit outside for awhile... Definitely need to do some test panels to see how it looks.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  5. #5
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Try looking at the following:

    http://www.artmetal.com/brambush/for...sages/732.html
    http://www.instructables.com/id/Very-Quick-rust/
    http://www.youtube.com/watch?v=8TNAxJXMzU8
    http://www.metalgeek.com/archives/2006/06/13/000065.php
    http://www.wikihow.com/Make-Metal-Rust

    Not saying the following will be feasible for you but saw a program on TV that discussed how they accelerate the "aging" process for Ford vehicles to test them before they hit the market.

    Salt bath
    Very high humidity (> 90%)
    High Temperature (122 F)
    Overnight
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  6. #6

    Default

    Get a bottle of regular Hydrogen Peroxide and after you scuff it to bare metal just "Paint" it on- Keep applying until you get the patina you want.
    Everlast PowerTig 200DX (Ordered-Waiting to arrive!)
    Everlast Supercut 50P


    Fortune Favors the bold.

  7. #7

    Default

    Vimegar will give you a flash rust.

  8. #8

    Default

    Quote Originally Posted by undercut View Post
    Try looking at the following:

    http://www.artmetal.com/brambush/for...sages/732.html
    http://www.instructables.com/id/Very-Quick-rust/
    http://www.youtube.com/watch?v=8TNAxJXMzU8
    http://www.metalgeek.com/archives/2006/06/13/000065.php
    http://www.wikihow.com/Make-Metal-Rust

    Not saying the following will be feasible for you but saw a program on TV that discussed how they accelerate the "aging" process for Ford vehicles to test them before they hit the market.

    Salt bath
    Very high humidity (> 90%)
    High Temperature (122 F)
    Overnight
    Thanks for all the links, helps out a bunch!

    "Sneak peek".... Started out as an idea when I put some cutoff's together...


    This is where I am right now.. This was just a test pic to make sure the scale of the front wheel was correct(It's not going to be a Flintstone mobile )
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  9. #9
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Cool idea! When I first read about your project, I wasn't quite sure what you had in mind. Nice to see there is some method to your madness! LOL Should turn out really nice. Good luck and cheers!
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  10. #10

    Default

    Yeah... I kind of fly by the seat of my pants sometimes..lol.

    This won't be to scale or anything but I'm working on the flat head V8 right now and I want to make a real looking radiator shell that will be polished. Just something to kill time when I'm not busy.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  11. #11

    Default

    Looks cool, cant wait to see how it turns out.
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

Similar Threads

  1. is multi process for me?
    By drthunder33 in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 01-23-2015, 01:33 AM
  2. Rust prevention tip
    By Rodsmachineshop in forum Tips & Tricks, Custom Tools, Safety, Ideas and Reviews.
    Replies: 18
    Last Post: 06-01-2012, 01:50 PM
  3. Project 3 from ogorir: floorpan/firewall rust repair
    By ogorir in forum On Road Fabrication
    Replies: 5
    Last Post: 10-25-2011, 05:48 AM
  4. Project #3 from Hooda- Electrolytic rust removal EXPERIMENT!
    By hooda in forum Personal Projects (no welder required)
    Replies: 21
    Last Post: 10-20-2011, 12:38 AM
  5. Project 1 from DaveO: electrolytic rust removal
    By DaveO in forum Personal Projects (no welder required)
    Replies: 15
    Last Post: 10-13-2011, 04:55 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •