Thread: Project 2 from Rambozo. Category: General Welding Repair

  1. #1
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Arrow Project 2 from Rambozo. Category: General Welding Repair

    Just a few repairs/modifications to a couple of trailers.
    This first one was a tilt bed that was made for a soil compactor, which I am repurposing to hold a golf cart utility vehicle. The center of gravity was not right to get the bed to drop unless the cart could drive on a little further. So I cut off the old stop, cut a couple of notches and added some wheel stops to let the cart come forward a few inches. Most all the welding was 6011 underneath and 7018 on the clean parts. I also welded on some brackets to attach some ratchet straps to tie down the cart, and a small hand winch to load the cart if it won't run.

    Click image for larger version. 

Name:	Projects 473.JPG 
Views:	555 
Size:	61.2 KB 
ID:	8199 Click image for larger version. 

Name:	Projects 475.JPG 
Views:	591 
Size:	64.8 KB 
ID:	8200 Click image for larger version. 

Name:	Projects 476.JPG 
Views:	584 
Size:	58.2 KB 
ID:	8201 Click image for larger version. 

Name:	Projects 477.JPG 
Views:	533 
Size:	55.8 KB 
ID:	8202 Click image for larger version. 

Name:	Projects 481.JPG 
Views:	570 
Size:	68.8 KB 
ID:	8203

    Click image for larger version. 

Name:	Projects 483.JPG 
Views:	595 
Size:	68.1 KB 
ID:	8204 Click image for larger version. 

Name:	Projects 485.JPG 
Views:	601 
Size:	69.1 KB 
ID:	8205 Click image for larger version. 

Name:	Projects 489.JPG 
Views:	603 
Size:	58.7 KB 
ID:	8206 Click image for larger version. 

Name:	Projects 523.JPG 
Views:	592 
Size:	61.6 KB 
ID:	8207 Click image for larger version. 

Name:	Projects 525.JPG 
Views:	635 
Size:	54.5 KB 
ID:	8208

    To be continued...
    Long arc, short arc, heliarc and in-the-dark!

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Arrow

    On another trailer I'm trying something new to protect the marker lights. I cut some 3" channel at an angle and used it as a guard for the lights. I also added a new coiled connector cord, which can be unplugged and swapped out when it gets damaged. As you may have guessed the workers who pull these are not the most careful people. It's not if they will break something, it's when.

    Click image for larger version. 

Name:	Projects 651.JPG 
Views:	553 
Size:	83.9 KB 
ID:	8210 Click image for larger version. 

Name:	Projects 653.JPG 
Views:	560 
Size:	65.1 KB 
ID:	8211 Click image for larger version. 

Name:	Projects 658.JPG 
Views:	550 
Size:	95.2 KB 
ID:	8209 Click image for larger version. 

Name:	Projects 654.JPG 
Views:	539 
Size:	97.9 KB 
ID:	8212 Click image for larger version. 

Name:	Projects 655.JPG 
Views:	588 
Size:	85.6 KB 
ID:	8213 Click image for larger version. 

Name:	Projects 656.JPG 
Views:	546 
Size:	78.7 KB 
ID:	8214
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Good idea on the marker lights with the angle cut channel. I always (now) box out the tail lights too.

    Nice mod on the first trailer as well. Hope no wood caught on fire.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  4. #4
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Yeah, I like the marker light protectors, too. I also like the thought you put into the center of balance. The new wheel stops look great! Cheers
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  5. #5
    Join Date
    Nov 2012
    Location
    Cambridge, ON. CA
    Posts
    111

    Default

    Wow. Keep it coming. These are some great ideas. I have an old camper that's been cut up and I want to convert it to a utility trailer. Needless to say those protectors could have come in handy when I backed the lights up into the fence last summer. Any more good ideas?

    I got a set of fender I've been meaning to put on as well but they've been sitting outside for a few months and are pretty nasty now. oh well.
    PowerArc 140ST
    Victor VPT-100FC

  6. #6
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    Looks good! I'll ditto the comments on the protectors. Quick, clean and easy, can't beat that.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

Similar Threads

  1. Project 3 from Rambozo. Category: General Welding Repair
    By Rambozo in forum Welding Repairs
    Replies: 2
    Last Post: 02-10-2013, 01:11 PM
  2. Project 2 from Youngnstudly. Category: General Welding Repair
    By youngnstudly in forum Welding Repairs
    Replies: 7
    Last Post: 02-01-2013, 05:34 AM
  3. Project#3 from CGCINC. Category: General Welding Repair
    By CGCINC in forum Welding Repairs
    Replies: 5
    Last Post: 12-11-2012, 06:33 PM
  4. Project 1 from Rambozo. Category: General Welding repair
    By Rambozo in forum Heavy Equipment and Commercial Projects
    Replies: 14
    Last Post: 08-01-2012, 12:45 AM
  5. Project 1 from CGCINC: Category: General welding repair
    By CGCINC in forum Welding Repairs
    Replies: 15
    Last Post: 07-17-2012, 02:24 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •