    I actually did this project on Sept 19, the second day I had my Supercut 50P.

    I used my PA140ST in TIG mode and SuperCut 50P. I was using a 3/32 2% thoriated with a #5 cap. Amperage was 140. Filler rod was a 1/16 ER70S2. The metal used was 6x4x.250 brick lentil.

    I used a piece of aluminum as a guide to cut the lentil. Amps were at 50 and pressure was approx 60. Cut like butter. I then changed caps for one without the guide and freehand cut at a 45 (just because it was thicker.... ) It measured .58 - .59 thick. I then used the plasma cutter to mark the holes and then drilled them on the press. All this drag tipping at 50 amps took a tole on the consumables... I then set the 140 at max and tacked the plate on. Once everthing looked good, welded top and bottom.

    Click image for larger version. 

Name:	lentle.jpg 
Views:	920 
Size:	126.2 KB 
ID:	8188Click image for larger version. 

Name:	guide.jpg 
Views:	970 
Size:	137.7 KB 
ID:	8187Click image for larger version. 

Name:	freehand.jpg 
Views:	942 
Size:	96.3 KB 
ID:	8186Click image for larger version. 

Name:	thickness.jpg 
Views:	971 
Size:	107.0 KB 
ID:	8184Click image for larger version. 

Name:	nozzle.jpg 
Views:	979 
Size:	127.3 KB 
ID:	8189Click image for larger version. 

Name:	bracket.jpg 
Views:	918 
Size:	147.1 KB 
ID:	8185Click image for larger version. 

Name:	rough-edge.jpg 
Views:	987 
Size:	142.1 KB 
ID:	8190Click image for larger version. 

Name:	rusty-weld.jpg 
Views:	1002 
Size:	145.9 KB 
ID:	8191

    I haven't had time to paint the bracket yet so it is already starting to rust.

    This was a easy project and didn't take long at all thanks to the SuperCut 50P. I am very happy with the results.
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

  2. #2

    Default

    what exactly is brick lentil and why use it on this?
    250 ex
    205 mig
    milwaukee grinder
    140e mig

  3. #3
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by johnson697 View Post
    what exactly is brick lentil and why use it on this?
    Think angle iron (although some are tee shaped). Lintel is used to support bricks across window or door openings.
    Long arc, short arc, heliarc and in-the-dark!

  4. #4

    Default

    learn something new everyday..i actually have a brick home with this angle iron in it .
    250 ex
    205 mig
    milwaukee grinder
    140e mig

  5. #5

    Default

    Yep it is basically angle iron. Only reason I used it on this is.... well it's what I had.
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

Similar Threads

  1. Project 2 from Rambozo. Category: Automotive On Road Trailer Jack
    By Rambozo in forum Other Custom Fabrications
    Replies: 5
    Last Post: 07-01-2015, 07:56 AM
  2. Replies: 28
    Last Post: 12-10-2012, 12:21 AM
  3. Project 1 from ShaneJackson. Category: Welding Cart
    By ShaneJackson in forum Other Custom Fabrications
    Replies: 27
    Last Post: 10-12-2012, 02:35 PM
  4. Replies: 18
    Last Post: 09-07-2012, 06:46 PM
  5. Project 2 from ShaneJackson. Category: General Welding repair
    By ShaneJackson in forum Welding Repairs
    Replies: 5
    Last Post: 09-01-2012, 06:15 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •