    Title says it all, really. There is a 1&1/4" pin that slides into a slot on the back of our fork lift. It's for light dragging as well as loading onto a vehicle using a winch. It's removable so you can use it with closed end shackles, etc. It's just hotrolled round bar with a handle welded on it. The rollback drivers often use it as a dead weight when respooling their winch lines, since using a birdsnested or otherwise FUBAR wire rope destroys it. Well, one driver didn't have the pin fully seated, and so the 8k winch bent the pin open, which made it non-removeable. I had a truck recovery early this AM, guy jack knifed in the rain, so was filthy and sweaty and soaking wet, so I didn't feel like getting into my car and going home til I air dried a little.

    Anyhow, I cut the pin out with a sawzall.Click image for larger version. 

Name:	2012-10-14_07-56-06_154.jpg 
Views:	474 
Size:	120.3 KB 
ID:	8175

    As you can see, it bent pretty easily over about a 8" unsupported length; it's dead soft mild steel.

    Click image for larger version. 

Name:	2012-10-14_07-56-15_304.jpg 
Views:	463 
Size:	103.3 KB 
ID:	8176

    So I played blacksmith and got out the cutting torch(no rosebud around) and between hammering with a sledge and pressing in a vise, I was able to straighten it out enough. I ground it into what was basically a giant V groove, so I could get access to the entire seection of the material.

    Then, I broke out the 160STH with the TIG and just started stacking the weld in at about 140amps, full power was too hot with just an on/off switch. Used 3/32" 70S2 filler, wound up extending it about 1", mostly to just wash out all the crap that I was getting off the pin.
    Click image for larger version. 

Name:	2012-10-14_10-44-34_304.jpg 
Views:	519 
Size:	127.8 KB 
ID:	8177

    Spent about 90 minutes on it, with about 10 minutes set up time for the welder, which I keep boxed up. More work than making a new pin, but no material costs. S/F.....Ken M
    Last edited by EchoSixMike; 10-14-2012 at 05:29 PM.
    Lincoln Power MIG 300
    Everlast 160STH
    Miller 225 Thunderbolt (sold it)
    Lincoln Squarewave 175 TIG(traded it for)
    Miller DEL 200 welder/genset
    Thermal Dynamics 1250XL plasma cutter
    Miller XMT300

  2. #2

    Default

    I suppose I should show a picture of the part doing it's job. Still a little tweaked, but does what it's supposed to

    Click image for larger version. 

Name:	2012-10-14_10-47-05_757.jpg 
Views:	477 
Size:	120.0 KB 
ID:	8180

    S/F.....Ken M
    Last edited by EchoSixMike; 10-14-2012 at 05:28 PM.
    Lincoln Power MIG 300
    Everlast 160STH
    Miller 225 Thunderbolt (sold it)
    Lincoln Squarewave 175 TIG(traded it for)
    Miller DEL 200 welder/genset
    Thermal Dynamics 1250XL plasma cutter
    Miller XMT300

Similar Threads

  1. Replies: 0
    Last Post: 09-10-2013, 07:23 PM
  2. 12" 200psi Antique Brass Pressure Gauge Repair
    By zoama in forum Personal Projects (no welder required)
    Replies: 12
    Last Post: 02-13-2013, 08:21 PM
  3. Northern Industrial 1644910 AD Helmet Opinions? (3.82" x 2.44" view area)
    By Welderooni in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 01-10-2013, 03:49 PM
  4. Cutting 3"x3"x3/16" Angle
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 7
    Last Post: 07-01-2011, 11:56 PM
  5. "Battlebot" Repair (TIG weld 4130 Cr-Mo steel)
    By jakeru in forum Welding Repairs
    Replies: 4
    Last Post: 03-07-2011, 09:51 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •