    Just tried my new 210ext was working good (I think) now it's doing this

    Any help would be appreciated
    210EXT,uni mig 250A, 200A inverter stick, 100A buzz box, 50A plasma cutter.
    If beef is in beef mince, What is in pet mince?

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Your settings would help?
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    100A 0 balance
    Click image for larger version. 

Name:	21ext.JPG 
Views:	630 
Size:	50.5 KB 
ID:	8174
    210EXT,uni mig 250A, 200A inverter stick, 100A buzz box, 50A plasma cutter.
    If beef is in beef mince, What is in pet mince?

  4. #4
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    There are a lot more settings than that. One drawback to a multi-function digital display is one pic will not show all the settings. Sine-wave is a lot less tolerant than square for dirty material in general. TIG is a lot different than stick and MIG, if you won't eat off it, it ain't clean enough for TIG. Make everything bright and shiny, and wipe it down with a solvent like acetone. Use a stainless brush dedicated to aluminum and carbide burrs instead of grinding discs.
    Last edited by Rambozo; 10-13-2012 at 11:46 PM.
    Long arc, short arc, heliarc and in-the-dark!

  5. #5

    Default

    Do you have a clean ground directly to the piece you're welding ?
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by zoama585 View Post
    Do you have a clean ground directly to the piece you're welding ?
    Looks marginal from the video. You can see the ground clamp, but the material is far from clean and no idea what that coating is. The fact that it does fire the main arc at some points and not others is a little odd.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7

    Default

    Quote Originally Posted by Rambozo View Post
    Looks marginal from the video. You can see the ground clamp, but the material is far from clean and no idea what that coating is. The fact that it does fire the main arc at some points and not others is a little odd.
    I see it now But the metal looks rusty.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  8. #8

    Default

    I tried it again after about a hour to cool and it's working again
    the metal is aluminum the stuff you can see is glue it is clean where I'm welding
    Maybe it just got to hot ?
    210EXT,uni mig 250A, 200A inverter stick, 100A buzz box, 50A plasma cutter.
    If beef is in beef mince, What is in pet mince?

Similar Threads

  1. 255 EXT Help, something went wrong with pulse
    By travis1693 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 09-20-2018, 10:11 AM
  2. 200DX, what am I doing wrong?
    By rappy'97 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 09-08-2015, 11:59 AM
  3. What am I doing wrong???
    By Toby in forum TIG Welding (GTAW/GTAW-P)
    Replies: 36
    Last Post: 04-09-2013, 12:54 AM
  4. wrong helmet sent
    By bubbas55 in forum Pre-sales, Sales and Shipping questions
    Replies: 1
    Last Post: 12-01-2012, 08:21 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •