Sharpie makes a silver metalic marker that works quite well. You can get them at most drugs stores and super stores. Two pack is like $3-4.
Also I use $.50 white grease pencils as well. Pick up black as well when you get the silver, for aluminum.
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.
The sharpie is great. I use those too. ( I have everything, even tungsten awl to scribe with). However, on new metal, the sharpie blends into the metal, though it does reflect light as a silvery glow when cutting.
Mark
performance@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x204
M-F 9am - 5pm EST
Good point Mark, yes I only use them to cut and grind.
Great idea on the tungsten awl. I have some unsed packs of green tipped tungsten electrodes that have been laying around.
[gripe] I was gonna just give them away since Praxxair would not take my "sealed" packages back as I did not have my receipt. What is sad for them was that it was the fellow I normally buy "all" my TIG and O/A consumables from (knows me, I bought them from him and they are the only locals that sell this brand), wanted to exchange them, they lost a good customer that day. But I am lucky enough to have Welder Supply and Lake Welding a little further up the road with better pricing I found.[/gripe]
Mike R.
Email: admineverlast@everlastwelders.com
www.everlastgenerators.com
www.everlastwelders.com
877-755-9353 x203
M-F 12 - 7PM PST
FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.