    I am considering the 250P. Howerver, I have several questions.

    1. It does not accept a spool gun. Which I am not a fan of anyway, but assuming it's a push gun that is supplied, are there any feeding issues when feeding softer alloys like 4043?

    2. Is it possible to adapt a push pull gun?

    3. I would be using the unit for aluminum mainly but would like to have the option for other metals. Is a liner kit available or would it be more practicle to purchase another gun?

  2. #2

    Default

    Metalux,

    I am sorry, but somehow this thread did not get answered. It happens sometimes, when we get interrupted, and have to leave the screen for a few minutes, as it won't show the thread under new threads anymore when we come back.


    A liner/ drive roll kit is available. Perhaps someone could adapt a spool gun, but you would have to tie into the circuitry.

    4043 should feed. I cannot say for sure as I haven't done any welding with it yet but that is what our factory has made it to do with the liners and 4 roll drives.

  3. #3

    Question

    This does not pertain to the posts prior to mine.

    With that said, I'd like to ask advice from Members or Support.


    I'm going to try welding a broken cast iron 2 way cross vise. I've already got my V channel ground.


    These would be my steps of operation:

    First, Heat both broken sections by placing them in cherry red coals in a metal 1/2 barrel from our wood stove (this should give me my 1100 F*).

    Second, Weld (flux core is only thing we've got) it while it's gently clamped in my bench vise.

    Then, Quickly replace it into the coals this will allow it to cool slowly, just letting the coals burn out.


    Thank you,
    I Love Plasma

  4. #4
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Default Noma-Cast Rod

    We're probably breaking some kind of protocol by putting this in the middle of another thread.
    My advice, take it or leave it. Stick weld it!
    There is a specialty rod called Noma-Cast, I have had VERY good luck with this rod, being a vice I assume looks aren’t a number one consideration.
    Hears a quote from the package.
    “Noma-Cast is specially developed for welding dirty, heat-affected, contaminated and oxidized cast iron where machinability is not required. Noma-Cast bonds to oil impregnated cast iron due to it’s non-conductive flux coating and nickel-free weld metal composition, it seals in porosity generating contaminates prior to finish welding with nickels. You can even use it to fill in large holes and join steel to cast material.”
    Check with your welding supply store.
    Just some advice from an old-timer, sometimes stick still is the way to go.
    Ray
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

  5. #5

    Default

    Thanx Ray. Not certain what I'll do yet.

  6. #6
    Join Date
    Jan 2010
    Location
    Chugiak , Alaska
    Posts
    259

    Post Noma-Cast rod

    Technical data if your at all interested.

    Tensile Strength – 62,000 PSI
    1/8” rod 70 - 125 Amps reverse polarity (DCEP)
    Made by Forney, (no I don’t work for them.)
    ____
    Ray

    Everlast Sales and Support Team.
    support@everlastalaska.com
    www.everlastalaska.com

    877-755-9353 X207

Similar Threads

  1. Pulsed Arc Welding?
    By scootarida1 in forum Stick Welding (SMAW)
    Replies: 5
    Last Post: 12-06-2012, 02:04 PM
  2. Excellent Pulsed TIG article
    By earla in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 08-25-2012, 02:49 AM
  3. Question about Pulsed Mig Process
    By Oxide00 in forum General Welder Questions
    Replies: 11
    Last Post: 03-20-2011, 01:23 AM
  4. practice pieces-Pulsed Tig
    By cdale2002 in forum Other Custom Fabrications
    Replies: 10
    Last Post: 07-30-2010, 01:15 PM
  5. Purchased 200 ACDC Pulsed
    By wallnut in forum Customer Testimonials
    Replies: 2
    Last Post: 05-01-2009, 01:54 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •