    Noticed this Argon bottle at my friends house also, it had a protective cap and built in regulator with a male quick coupler already installed .Hose from his Metabo mig plugged right into the bottle.

    Click image for larger version. 

Name:	Argon Bottle.jpg 
Views:	513 
Size:	138.0 KB 
ID:	8153
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  2. #2
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    Does the shroud thread onto the cylinder cap threads? I'm trying to figure out that flattened up shape on top, thought maybe a lifting handle but probably not if the shroud is plastic.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  3. #3

    Default

    That is really interesting... I have never seen anything like that. Built in regulator??? Wonder how they fill it??
    Shade tree MIG welder.
    Now a Shade tree TIG welder.

  4. #4
    Join Date
    Oct 2010
    Location
    Northern Virginia
    Posts
    1,323

    Default

    I was thinking the regulator and the shroud belong to the customer, and that they fill and ship bottles as you'd expect but that the user / owner attaches that... thing... when he gets it to his shop. But when I look at the photo, that barbed nipple sticks out a little, and it looks like in a bad enough roll-over accident the nipple could be bent, and isn't that what the shroud is trying to prevent?! So I don't think I'm getting it.
    DaveO
    Oxweld oxy acet gear
    IMIG 200
    PowerTIG 210 EXT... Amazing!

  5. #5
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    I don't think that shroud is user installed, it looks like the valve handle would get in the way of unscrewing. If that is a carrying handle on top, it sure looks handy.

    I wonder how the guy gets it filled over here.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  6. #6
    Join Date
    Feb 2012
    Location
    Indian Shores Beach, FL - U.S.A.
    Posts
    101

    Default

    It appears to be a two piece bolt together shroud similar to the ones used for oxygen tanks in the medical industry.
    PowerTig 250EXT ordered on 2/20/12 - AluMig~250P - MasterTig~250AC - Matco Mig~Spot Welder - Giaintec CAT250D - Harris Steelworker Oxy/Acet - Henrob DHC 2000 - Van Norman CB1401 - Lagun FTV1 Mill - CM Mill/Drill - CM 13x40 Lathe - CM 7x12 Bandsaw - CM 6x48 Belt Sander - CM 12 Disc Sander - Baldor 3/4HP Buffer - TP 960 Blast Cab - 48~Box & Pan Break - 52~Foot Shear - 20~Ton Press - 80~Gal 7.5HP Compressor - 9' Snap On Tool Box - 30' Stainless Tool Box Workbench - 3M Speedglas 9100Xx

  7. #7
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Europeans always get the good stuff. I've seen some awfully nice looking European flowmeters that have a knob for adjusting pressure in addition to the usual knob for adjusting flow. Wish we had that style in the US, but all I've ever seen around here (and that fit our bottles) are single adjustable flowmeters.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  8. #8

    Default

    Quote Originally Posted by jakeru View Post
    Europeans always get the good stuff. I've seen some awfully nice looking European flowmeters that have a knob for adjusting pressure in addition to the usual knob for adjusting flow. Wish we had that style in the US, but all I've ever seen around here (and that fit our bottles) are single adjustable flowmeters.
    The bottle comes like that from the distributor, He had an extra one in his shop. It is the protective cap and handle together.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

  9. #9

    Default

    If a regulator ever "blows" it is definitely a smart idea. Also if the cylinder ever falls over, unchained, it'll keep the cylinder from becoming a V-2.

  10. #10
    Join Date
    Feb 2012
    Location
    Indian Shores Beach, FL - U.S.A.
    Posts
    101

    Default

    They're several different types of gas cylinder protectors available in the US market but none seemed to guard the regulators too well.


    PowerTig 250EXT ordered on 2/20/12 - AluMig~250P - MasterTig~250AC - Matco Mig~Spot Welder - Giaintec CAT250D - Harris Steelworker Oxy/Acet - Henrob DHC 2000 - Van Norman CB1401 - Lagun FTV1 Mill - CM Mill/Drill - CM 13x40 Lathe - CM 7x12 Bandsaw - CM 6x48 Belt Sander - CM 12 Disc Sander - Baldor 3/4HP Buffer - TP 960 Blast Cab - 48~Box & Pan Break - 52~Foot Shear - 20~Ton Press - 80~Gal 7.5HP Compressor - 9' Snap On Tool Box - 30' Stainless Tool Box Workbench - 3M Speedglas 9100Xx

  11. #11
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    It is somewhat understandable with all the different types of regulators. You would have to go with a standard like that German cylinder, or each regulator manufacturer would have to make their own style guard. If you follow proper safety rules by only attaching regulators to secured cylinders, the falling over risk is reduced, but things could still fall on the exposed regulator and break something. I'm sure that would defeat some cylinder securing methods I've seen used. But most should contain the tank as it empties. The one constant is that there is no guard for stupid. I'm sure there are some people that would find a way to make that German cylinder fly around the shop.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. 17 style 25' Tig Torch From Everlast ??
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 01-25-2013, 06:17 PM
  2. WP-18 15' Water Cooled Tig Torch Available and What Style
    By cbmkr in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 12-20-2012, 05:07 PM
  3. Need Argon Bottle Wondering What's Fair
    By Slartybartfa in forum General Welder Questions
    Replies: 16
    Last Post: 06-01-2012, 01:16 AM
  4. New forum style for those with worse eyes that me
    By everlastsupport in forum Forum related Questions
    Replies: 16
    Last Post: 02-23-2011, 02:40 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •