Share
Results 1 to 20 of 25

Thread: Noob's first beads with 140st- problem with 110

Threaded View

Previous Post Previous Post   Next Post Next Post
  1. Default Noob's first beads with 140st- problem with 110

    I got my 6-50 plug wired to my new 140st today, and also made a whip to use 110. Chopped up a piece of 1/8" angle I had and ran a few beads before I had to quit due to storm clouds. I have to weld outside, so the weather is always a consideration. I have an old stainless food service table as my bench.

    I had a handful of Lincoln 6013 rods and some Horrible Freight 6011. Besides the slag coming off the 6013 more easily, they burned pretty similarly.

    I think there was a little improvement from my first beads to my last, and I even managed a couple lap joints. Penetration looked good from the edges (to my noob eyes).

    I'm really impressed so far with the little 140. My only problem was I could not get the 110 to light up at all. On 220 both rods lit up like a kitchen match, all the way down to 60 amps. At 110 amps I was cutting pieces off a 3/16" bar with the 6011.

    I tried the 110 circuit with the work clamp grounded to the table and directly to the angle. Nuthin'.

    I made a whip with 10/3 left over from an extension cord. I'm sure the polarity is correct. Using the 110 whip in a 20 amp outlet, the welder amp display lights up, but I can't get an arc to strike. What can I check? Help!

    Below are some pics:




    Last edited by MotoJ; 10-06-2012 at 07:12 PM.

Similar Threads

  1. Please critique these beads
    By JohnT in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 07-31-2014, 09:11 PM
  2. My opinions on the PowerTig 250EX (so far) and first beads..
    By tom_tom in forum Customer Testimonials
    Replies: 3
    Last Post: 01-02-2014, 06:48 AM
  3. iTig-200 Noob having some troubles doing beads on 1/8
    By seanm in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 03-10-2013, 07:23 PM
  4. First beads on a PowerArc 140ST
    By MuttonHawg in forum Customer Testimonials
    Replies: 30
    Last Post: 02-25-2013, 09:28 PM
  5. A couple of beads from my new mig
    By A/C Guy in forum General Welding Questions
    Replies: 7
    Last Post: 04-09-2011, 07:08 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •