Share
Page 2 of 2 FirstFirst 12
Results 21 to 25 of 25

Thread: Noob's first beads with 140st- problem with 110

  1. Default

    Thanks Rambozo,

    This is what I've got: white wire from welder to narrow blade on 5-60, black to wide, green ground. At the whip, when plugged into 110 outlet, 5-60 receptacle on the end has narrow hole to ground at 0 volts, wide to ground is 120, 120 across narrow and wide. When I plug the welder into the whip, no change from before.

    I took the 5-60 off and installed a 5-15- white to silver, black to gold, green ground. Corresponding outlet has 0 volts on wide blade, 120 narrow. That's correct, yeah?

    Still no change. I never had it plugged in for more than seconds. I don't think it would fry instantaneously. With the 220 plug back on, it strikes easy and welds great.

  2. #22
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by MotoJ View Post
    I took the 5-60 off and installed a 5-15- white to silver, black to gold, green ground. Corresponding outlet has 0 volts on wide blade, 120 narrow. That's correct, yeah?
    Yup, that's right.

    ...I don't think it would fry instantaneously...
    I hope those aren't famous last words. There are plenty of electronic devices that do fry instantly. I'm sure someone from Everlast support will know as I'm sure they have seen this before.
    Because of the warning in the manual and a few others mentioned on this forum, I built my plug with a built in tester to make sure it never happend to me, in case I ran into an outlet wired wrong.

    Also I'm guessing you meant 6-50 not 5-60.
    Last edited by Rambozo; 10-07-2012 at 07:39 PM.
    Long arc, short arc, heliarc and in-the-dark!

  3. Default

    I hope that's not the case they can get zapped that easy. In that case, if you plugged your cord in and the tester showed the outlet was bad, wouldn't it already be too late?
    Last edited by MotoJ; 10-07-2012 at 07:43 PM.

  4. #24
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by MotoJ View Post
    I hope that's not the case they can get zapped that easy. In that case, if you plugged your cord in and the tester showed the outlet was bad, wouldn't it already be too late?
    Not if I don't flip the power switch.

    Since it still works on 240V it can't be that bad, maybe something simple in the auto voltage switching.
    Last edited by Rambozo; 10-07-2012 at 07:47 PM.
    Long arc, short arc, heliarc and in-the-dark!

  5. Default

    Man I hope so. I could use some good luck lately. Thanks for seeing me through this snafu!

Similar Threads

  1. Please critique these beads
    By JohnT in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 07-31-2014, 08:11 PM
  2. My opinions on the PowerTig 250EX (so far) and first beads..
    By tom_tom in forum Customer Testimonials
    Replies: 3
    Last Post: 01-02-2014, 05:48 AM
  3. iTig-200 Noob having some troubles doing beads on 1/8
    By seanm in forum TIG Welding (GTAW/GTAW-P)
    Replies: 18
    Last Post: 03-10-2013, 06:23 PM
  4. First beads on a PowerArc 140ST
    By MuttonHawg in forum Customer Testimonials
    Replies: 30
    Last Post: 02-25-2013, 08:28 PM
  5. A couple of beads from my new mig
    By A/C Guy in forum General Welding Questions
    Replies: 7
    Last Post: 04-09-2011, 06:08 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •