  1. #1

    Default How Bad is this tip/electrode

    How do you tell when to change the tip and electrode.

    I think this tip/electrode set is bad. Is that right, and how bad is it?

    Thanks.


    Click image for larger version. 

Name:	electrode.jpg 
Views:	497 
Size:	95.1 KB 
ID:	8099Click image for larger version. 

Name:	tip.jpg 
Views:	473 
Size:	51.6 KB 
ID:	8100
    Just starting in Aug '10
    ---
    Hobart Handler 187
    Power Plasma 50

  2. #2

    Default

    Quote Originally Posted by EmptyNester View Post
    How do you tell when to change the tip and electrode.

    I think this tip/electrode set is bad. Is that right, and how bad is it?

    Thanks.


    Click image for larger version. 

Name:	electrode.jpg 
Views:	497 
Size:	95.1 KB 
ID:	8099Click image for larger version. 

Name:	tip.jpg 
Views:	473 
Size:	51.6 KB 
ID:	8100
    A tip is only bad when it doesn't cut right,,,just looking at a tip is somewhat misleading,,that tip could have lot's of miles left in it.
    Some of those lies people tell about me, are true

  3. #3

    Default

    Hole elongation is the primary wear you are looking for.

  4. #4
    Join Date
    Mar 2011
    Location
    Eastern Oregon
    Posts
    681

    Default

    What effect does the cratering at the end of the electrode have? I normally replace mine at the same time just because they are sets, but other than discoloration, they seem to hold up much better than the tips.
    Penncrest Buzzbox - Infinite amp control! Man the 70's were good.
    Everlast Powerplasma 60 - Reliable unit, cuts well.
    Everlast i-MIG 250P w/spoolgun - Really smooth, plenty of cajones.
    Everlast 250EXT - Sometimes it just takes a kick in the balls...
    Everlast 255EXT - Just started playing

  5. #5

    Default

    Quote Originally Posted by performance View Post
    Hole elongation is the primary wear you are looking for.
    By elongation do you mean "depth" or "diameter"?
    Just starting in Aug '10
    ---
    Hobart Handler 187
    Power Plasma 50

  6. #6

    Default

    Elongation would refer to the diameter.

Similar Threads

  1. Stick electrode holder
    By joshuab in forum Other Custom Fabrications
    Replies: 11
    Last Post: 08-04-2013, 11:16 AM
  2. Electrode Guide?
    By Columbo in forum Stick Welding (SMAW)
    Replies: 14
    Last Post: 03-21-2013, 11:20 PM
  3. Electrode
    By Buggy Chief in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 03-31-2012, 03:28 PM
  4. electrode holder
    By bobwills in forum General Welder Questions
    Replies: 5
    Last Post: 12-24-2011, 08:30 PM
  5. DIY Tig Electrode sharpener
    By acourtjester in forum Other Custom Fabrications
    Replies: 4
    Last Post: 06-10-2011, 02:20 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •