Share
Results 1 to 10 of 10

Thread: PowerPro 256 AC Not Working

  1. #1

    Default PowerPro 256 AC Not Working

    Set up to weld some .25 aluminum but I only get a quiet DC arc. Sounds exactly like welding steel and no cleaning action at all. I've checked and recheck settings, flipped the ac/dc switch back and forth, moved the ac balance around but no change. It's putting out the amps and melts the aluminum with ease. When I flip the switch from AC to DC the display drops a few amps. When I put it back to AC the display reads the number I set for AC again so all that seems normal.
    Settings, Pulse off, 180 amp, switch to AC, freq and balance at 2 and 10, HF, Tig, 2T with the pedal, pre flow 1, post flow 6, torch in negative, clean new 6061 aluminum .25"

    It's gotta be something simple.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  2. #2
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Since you can't turn off the HF, it might not be such a good idea to measure the output with a voltmeter to confirm that it's DC. You can go to stick mode in AC and measure the outputs to see if it's DC only.
    Last edited by Rambozo; 09-20-2012 at 03:24 AM. Reason: Answered my own question buried in manual
    Long arc, short arc, heliarc and in-the-dark!

  3. #3

    Default

    Quote Originally Posted by Rambozo View Post
    Since you can't turn off the HF, it might not be such a good idea to measure the output with a voltmeter to confirm that it's DC. You can go to stick mode in AC and measure the outputs to see if it's DC only.
    The arc is very quiet with no cleaning action at all.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  4. #4

    Default

    Check under the cover toward the front of the top board and make sure all your plugs are firmly seated.

  5. #5

    Default

    Quote Originally Posted by Rambozo View Post
    Since you can't turn off the HF, it might not be such a good idea to measure the output with a voltmeter to confirm that it's DC. You can go to stick mode in AC and measure the outputs to see if it's DC only.
    Actually, not all PP256's will do AC in stick mode ... mine does not.

    Cheers
    Mike
    Power Pro 256

  6. #6
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by posixPilot View Post
    Actually, not all PP256's will do AC in stick mode ... mine does not.

    Cheers
    Mike
    Boo. I was wondering about that and had to go through the manual since it wasn't listed in the specs. Of course I looked at the newest version of the manual. I know there have been some changes. Do you have the CNC port?
    Not that I would use it much, but there are times where AC for stick is nice. I bet with the right settings you could probably do stick with the machine set in TIG mode if you really needed to. I know I used a foot pedal once for stick welding where all I had was my TIG machine. It worked rather well as I had some really messed up torch cut and rusted away steel to do vertical welds on with a horrible fitup and lots of gaps to fill with 6011. Having HF start for stick almost felt like cheating, too.
    Long arc, short arc, heliarc and in-the-dark!

  7. #7

    Default

    Quote Originally Posted by Rambozo View Post
    Boo. I was wondering about that and had to go through the manual since it wasn't listed in the specs.
    Yeah, the website actually listed AC SMAW until a couple of months ago, so you are in good company . Mine does have the CNC port, but doesn't appear to weld in AC/stick ... when I tried it the arc and weld quality was identical to DC.

    Cheers
    Mike
    Power Pro 256

  8. #8

    Default

    Quote Originally Posted by performance View Post
    Check under the cover toward the front of the top board and make sure all your plugs are firmly seated.
    Just got a chance to work on it this morning. I pulled the cover and checked the plugs... never felt one seat any further but I fired it up and AC is working again.
    Thanks for the help.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  9. #9
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Glad to hear you're back in business. It always bugs me when I can't find the problem and something fixes itself.
    Long arc, short arc, heliarc and in-the-dark!

  10. #10

    Default

    Quote Originally Posted by zoama585 View Post
    Just got a chance to work on it this morning. I pulled the cover and checked the plugs... never felt one seat any further but I fired it up and AC is working again.
    Thanks for the help.
    Probably a loose wire in the plug then.

Similar Threads

  1. Plasma stopped working on PowerPro 205
    By mak in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 12
    Last Post: 10-12-2020, 12:29 AM
  2. My 256 AMP display is not working.
    By jim wilson in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 8
    Last Post: 07-12-2018, 03:10 PM
  3. PP256 HF not Working... Again
    By greygizmo in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 16
    Last Post: 07-19-2016, 02:45 AM
  4. 20 years later and still working on it
    By braveops in forum Truck, Car and Bike builds
    Replies: 7
    Last Post: 06-01-2016, 06:08 AM
  5. Plasma not working
    By Greg in forum Everlast Plasma Cutters (PAC)
    Replies: 14
    Last Post: 11-25-2009, 05:23 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •