Share
Results 1 to 12 of 12

Thread: First time using gas lens...wow!

Hybrid View

Previous Post Previous Post   Next Post Next Post
  1. #1

    Talking First time using gas lens...wow!

    I bought some gas lenses for my torch and all I have to say is wow! I had to weld a cap on some mild steel tube today. Did a fusion weld. The arc was very stable and I was able to get 1/2" stick out so I could see what I was doing. It made me a better welder. I don't know why anyone would use a normal collet.

  2. #2

    Default

    They are available in very large 12 and 15 sizes as well. They consume much more argon though when they are very large.

    You can also get extended length cups for the gas lens setups, sometimes allowing you better access if it is tight.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  3. #3

    Default

    Cool, I haven't gotten to tig yet with my 256 because I don't have a water cooler. Tomorrow I should get my new CK air cooled torch and be ready to light up. I opted to get their gas saver front end for it with the pyrex cover just because being able to see more will probably help me learn to tig faster. If all the hype is true, I'll get improved shielding and be able to turn the flow down a little.
    PowerPro 256, Lincoln Electric Weld Pack, 220V HF Spot welder,
    RF45 Mill/Drill(clone), and more $$$ in tooling for the mill than it's worth!
    Cadillac 14 x 40 lathe (not yet running)

  4. #4

    Default

    Quote Originally Posted by hobbymachnst View Post
    Cool, I haven't gotten to tig yet with my 256 because I don't have a water cooler. Tomorrow I should get my new CK air cooled torch and be ready to light up. I opted to get their gas saver front end for it with the pyrex cover just because being able to see more will probably help me learn to tig faster. If all the hype is true, I'll get improved shielding and be able to turn the flow down a little.
    You can just hook up the torch to a garden hose with some extra rubber hose, a few hose clamps, and a place to let the water drain. It doesn't take much.
    Everlast 200DX
    Everlast PT185
    Shoptask 3-in-1 (not currently in my garage, but I own it...)

    Any day on a motorcycle like this that ends just needing parts and labor is a good day.
    4.82, 158.67mph 1/8th mile 7.350, 200.35mph 1/4 mile

  5. #5

    Default

    Quote Originally Posted by sportbike View Post
    You can just hook up the torch to a garden hose with some extra rubber hose, a few hose clamps, and a place to let the water drain. It doesn't take much.
    I thought I might be able to do that, in fact I considered hooking up my flood coolant pump to the thing just to have some fun, but plasma cutting and stick welding kept me busy until today... I lit up the tig today. I didn't have time to do much but destroy a little piece of aluminum, but it was fun.
    PowerPro 256, Lincoln Electric Weld Pack, 220V HF Spot welder,
    RF45 Mill/Drill(clone), and more $$$ in tooling for the mill than it's worth!
    Cadillac 14 x 40 lathe (not yet running)

  6. #6

    Default

    Quote Originally Posted by hobbymachnst View Post
    Cool, I haven't gotten to tig yet with my 256 because I don't have a water cooler. Tomorrow I should get my new CK air cooled torch and be ready to light up. I opted to get their gas saver front end for it with the pyrex cover just because being able to see more will probably help me learn to tig faster. If all the hype is true, I'll get improved shielding and be able to turn the flow down a little.
    I just use the hose for water cooling. I don't weld enough to justify a water cooler. It's also nice cause as a beginner welder I tend to need to sharpen the tungsten a lot due to contamination and it's instantly cool.

  7. #7
    Join Date
    Dec 2009
    Location
    Greater Seattle, WA
    Posts
    813

    Default

    Quote Originally Posted by Ron66 View Post
    I don't know why anyone would use a normal collet.
    If you're welding something dirty, like galvanized steel, or material where the back side can't be cleaned, the contaminants can boil, pop, etc onto your metal screens, and ruin them in a gas lens. IME, those are good situations for using a standard collet body.
    '13 Everlast 255EXT
    '07 Everlast Super200P

  8. Default

    Slightly off topic here but, with galvanized metal, you should grind off all the plating within about an inch of the weld area. The zinc in the plating boils off and if inhaled, will put you in the hospital with some pretty serious lung issues and will contaminate your body with hundreds of times more zinc that it's prepared to deal with -much akin to lead poisoning. If you've ever stick welded galvanized metal (where the heat is much more intense) that white powder that coats everything is pure zinc...


    Quote Originally Posted by jakeru View Post
    If you're welding something dirty, like galvanized steel, or material where the back side can't be cleaned, the contaminants can boil, pop, etc onto your metal screens, and ruin them in a gas lens. IME, those are good situations for using a standard collet body.

  9. #9
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by Ron66 View Post
    I don't know why anyone would use a normal collet.
    The gas lens cups are a lot larger in diameter than a standard 9/20, so for some tight places it won't fit, extra stickout or not.

    Quote Originally Posted by Ray C View Post
    Slightly off topic here but, with galvanized metal, you should grind off all the plating within about an inch of the weld area. The zinc in the plating boils off and if inhaled, will put you in the hospital with some pretty serious lung issues and will contaminate your body with hundreds of times more zinc that it's prepared to deal with -much akin to lead poisoning. If you've ever stick welded galvanized metal (where the heat is much more intense) that white powder that coats everything is pure zinc...
    It's always a good idea to wear a respirator especially around galvanizing. For example if you are welding galvanized pipe, you may have ground it all off the outside, but it can still boil up from the inside where you might not have access to grind. And to get back on topic, it can then pop up into your weld puddle and ruin your gas lens screen.
    Long arc, short arc, heliarc and in-the-dark!

  10. #10

    Default

    I didn't know the gas lens would make that much of a difference. It does make sense that it would consume more Argon for the given area I guess. I hadn't really thought of that before. Sort of sounds like use them when needed, but otherwise select the best standard cup for the use?
    Miller 210 MIG
    Eagle 3-Cylinder Compressor
    Air Tools
    Body Tools, Shrinker, Stretcher
    Bead Blast Cabinet
    Homebuilt Car Rotisserie

    1971 Dodge Challenger, Pro-Touring, 6.1 Hemi, Fikse Wheels, 335/275 Tires (in progress)

  11. #11
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by MoparCar View Post
    I didn't know the gas lens would make that much of a difference. It does make sense that it would consume more Argon for the given area I guess. I hadn't really thought of that before. Sort of sounds like use them when needed, but otherwise select the best standard cup for the use?
    It always comes back to the same thing; Use the right tool for the job.
    Long arc, short arc, heliarc and in-the-dark!

Similar Threads

  1. Gas Lens Question
    By MCoupe in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 02-20-2014, 03:07 PM
  2. Changing to a gas lens what do I need.
    By PeterA in forum TIG Welding (GTAW/GTAW-P)
    Replies: 7
    Last Post: 11-09-2012, 05:56 PM
  3. Anyone using a gas lens?
    By HemiRod23 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 07-23-2012, 06:16 PM
  4. Lens # choice?
    By Trip59 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 36
    Last Post: 06-06-2012, 06:30 PM
  5. Gas lens?
    By Buggy Chief in forum TIG Welding (GTAW/GTAW-P)
    Replies: 28
    Last Post: 02-27-2012, 09:09 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •