    Default PowerPlasma 80 Question

    I have had the PowerPlasma 60 for a year or so, and am pretty happy with it. I went with the 60 instead of the 80 because for some reason I thought the 80 was a three phase unit. I do not have three phase power in my garage so I went with the 60. I have a friend who was looking at buying a Plasma so I loaned him mine. Now I have an opporunity to sell it to him and am considering doing so. I am running a 50 amp breaker, on my power. Looking for any thoughts on the upgrade, anyone using an 80 currently?
    _________________________________________
    Everlast PowerPlasma 60
    Everlast 250EX w/ Cooler
    Lincoln PowerMig 256
    Lincoln 250LX spool gun
    JD2 Model 32 bender

  2. #2

    Default

    I would only run the PP80 on 3 phase myself. I have a PP60, I have owned 50/60/70. Going back to a PP70, but that will be the limit for me. 80 and 100 like 3 phase a lot better.

    The PP50 is a slick little unit if you like the smaller size but almost all the power.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  3. #3

    Default

    80 3 phase only in Canada. 1 phase here though some have been ordered 1 and 3 phase (dual phase) here. Not sure what is currently available and in stock on that , but 1 phase will get you by...but you're going to need 70 amps.

  4. #4

    Default

    Quote Originally Posted by performance View Post
    80 3 phase only in Canada. 1 phase here though some have been ordered 1 and 3 phase (dual phase) here. Not sure what is currently available and in stock on that , but 1 phase will get you by...but you're going to need 70 amps.
    That was my point, if I did not have 3 phase I would not run the PP80 due to the current required to run it. PP70 is the larger unless I had 3 phase..
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  5. #5

    Default

    I have the 80 and running on 50 amps single phase is no problem,,,just remember the rule of thumb for plasma's,,the power in will only give you 10 more amps of plasma than the breaker,,,to get 80 amps plasma you need a 70 amp breaker, ,,,for 70 amps of plasma you need a 60 amp breaker and so forth,,Nothing wrong with having a bigger plasma,,,cause some days I may hook it up to the 3phase or maybe just install a 70 amp breaker on the short run welding plug...the welding plug closest to the breaker box ( 3 feet away) has a 60 amp breaker on it,,,so I can pull 70 amps on my PP80
    Some of those lies people tell about me, are true

Similar Threads

  1. Quick question regarding Powerplasma 50
    By Rupes in forum Everlast Plasma Cutters (PAC)
    Replies: 8
    Last Post: 03-29-2014, 05:22 PM
  2. Powerplasma 50
    By trickbiker in forum Customer Testimonials
    Replies: 1
    Last Post: 10-03-2011, 03:18 AM
  3. Question about PowerPlasma torches
    By Scooter in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 03-26-2011, 01:15 PM
  4. PowerPlasma 50
    By AMDninjaboy in forum Everlast Plasma Cutters (PAC)
    Replies: 0
    Last Post: 11-22-2010, 01:25 PM
  5. The New Powerplasma 50 question
    By Kapoor in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 01-16-2010, 06:48 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •