Share
Results 1 to 3 of 3

Thread: Practicing with my 140ST

  1. #1

    Default Practicing with my 140ST

    So I finally got a chance to try out my new Tillman gloves today. I tried both the 25's and the 44's. I like the 44's just a little better than the 25's. I like the cuffs on the 44's better but like the feel of the 25's better, but once you start welding there isn't much difference.

    Anyways, first thing I tried was a little aluminum and DCEP.... The aluminum I was using was anodized picture framing. I didn't bother cleaning off the anodized coating... needless to say it wasn't too pretty. On the places where I burnt off the anodized coating, I went back and added filler... actually didn't look terribly bad.

    After that experiment I grabbed some scrap steel. It was .11 thick and I set the 140ST to 60 amps. Here is a picture:

    Click image for larger version. 

Name:	practice.jpg 
Views:	457 
Size:	146.4 KB 
ID:	7816

    Considering this is the 3rd time I have welded Steel with TIG, I am not too ashamed with the results. I have a small section that has the stacked coins look.... One thing I did notice is on that section, the back side does not have full penetration like the rest. I am guessing I should have been higher on the amps and a faster travel speed?
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

  2. #2
    Join Date
    Apr 2012
    Location
    Washington State
    Posts
    723

    Default

    Are you sure that was only your third try at steel tig welding? Looks pretty good and it looks like you've got an eye on what to look for to improve on.

    Anodized aluminum without cleaning the coating huh! That'll teach ya!

    I'm curious how much success you're going to have welding aluminum with straight DC. 100% cleaning will put a lot of heat on the tungsten. Look forward to hearing how well that works for you.

    Sounds like you are having fun with your 140st. It's a really nice, compact and capable unit!

    Cheers
    Is it OK to want to break something just so that you can weld it back together?

    Everlast PowerTIG 185 Micro IGBT AC/DC Welder

  3. #3

    Default

    Yep that was my 3rd time. So was I right on what I needed to do to improve?

    As far as aluminum, I was just playing to see what it would do. And you are right the tungsten melted a lot and formed a huge ball on the end.

    I am having fun with the 140ST, only thing I really wish it had was a foot pedal.
    Everlast PowerTig 200DX
    Everlast Supercut 50P
    I need a MIG.... which one to buy:
    I-Mig 160, I-Mig 200, or a MTS 160

Similar Threads

  1. TIG - Practicing beads on mild steel, getting a bump at the end
    By seanm in forum General Welding Questions
    Replies: 3
    Last Post: 02-15-2014, 03:50 PM
  2. Been practicing on some aluminum...
    By blasphemy000 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 4
    Last Post: 11-12-2012, 01:19 PM
  3. Power Arc 140ST
    By valveman in forum General Welder Questions
    Replies: 47
    Last Post: 05-01-2012, 05:51 AM
  4. Power Arc 140ST
    By valveman in forum Buy, Sale or Trade
    Replies: 2
    Last Post: 02-05-2012, 12:24 PM
  5. Power Arc 140st
    By SeanMurphy265 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 3
    Last Post: 06-16-2011, 11:14 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •