    Hi All
    I did some mods to the foot pedal that came with my PM 256. I read that other guys had probems with the timing belt shaft getting off the pot and not working. See attached pictures. I made 2 brackets on of 1/4" X 1" X 1" angle about 1-1/2" long and the other is 1/8" flat cut to shape and bent to a 90.
    I used 10-32 screws and nuts to hold them on. The 1/4" bracket has a tongue that sticks info the back of the timing belt shaft as a guide.

    Have fun
    acourtjester
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	DSCF4101.JPG 
Views:	803 
Size:	65.1 KB 
ID:	243   Click image for larger version. 

Name:	DSCF4106.jpg 
Views:	856 
Size:	88.5 KB 
ID:	244   Click image for larger version. 

Name:	DSCF4109.jpg 
Views:	870 
Size:	86.4 KB 
ID:	245  

Similar Threads

  1. 250 EX Foot pedal
    By Dick Eue in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 09-27-2018, 04:49 PM
  2. Foot pedal mods for PA160-STH
    By joshuab in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 21
    Last Post: 08-21-2013, 05:43 PM
  3. Foot Pedal Fix
    By Ron66 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 03-26-2012, 12:29 AM
  4. new foot pedal
    By hesstx in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 12-16-2011, 05:26 PM
  5. Bad foot pedal?
    By sth212 in forum TIG Welding (GTAW/GTAW-P)
    Replies: 6
    Last Post: 08-21-2011, 08:50 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •