Share
Results 1 to 20 of 20

Thread: Just recieved my drag tips today!!

  1. #1

    Default Just recieved my drag tips today!!

    I bought some drag tips for my PP50, got them here...
    http://www.ebay.com/itm/10PC-PLASMA-...item27b730d822

    I hate the cheap wire standoff that comes with the torch and after using a friends Hypertherm 1250 with drag tips I decided to try them on my cutter.
    I LIKEY!!! Seems easier to cut with and I get cleaner and faster cuts! Hopefully these will let me do some freehand work easier.
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  2. #2

    Default

    take some pics of some cuts want to see how they work and cut . yes the wire stand off that comes with torch always get welded or catches on stuff
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  3. Default

    So do drag tips wear quicker since they are dragging on the metal when hot or just like the other ones or better.
    Gabe
    everlast power arc 200
    Lincoln electric 225 tombstone
    lawn mowers

  4. #4

    Default

    That guy...hmm. He's the one on WW that is constantly creating controversy for us and seems to be a know it all and a source of misinformation about our product. Not that you shouldn't buy from him, but beware of his motivation and intent.

    There are a number of places you can get those tips. HTP for one, with a better reputation and they use genuine trafimet or extremely better quality than the average guy. http://www.usaweld.com/Parts-for-Mic...-625-parts.htm
    Also, Weldmart.com has them.
    http://www.weldmart.com/store/RTS-4700.htm

    For a cheap source as good as or better than what you found for the future:
    http://www.ebay.com/itm/10pcs-Tips-1...item5d2f944ffc

    You can get a rolling standoff from us for that torch.

    A thing about those consumables...They probably won't have the wear life...because they are made from inferior chinese recycled copper which has a high tin content which wears much faster. The ones we send with the torch are genuine trafimet, and our replacements use copper made and sourced from Finland...There's a big difference in wear.
    Last edited by performance; 08-22-2012 at 11:48 AM.

  5. #5

    Default

    Quote Originally Posted by performance View Post
    That guy...hmm. He's the one on WW that is constantly creating controversy for us and seems to be a know it all and a source of misinformation about our product. Not that you shouldn't buy from him, but beware of his motivation and intent.

    There are a number of places you can get those tips. HTP for one, with a better reputation and they use genuine trafimet or extremely better quality than the average guy. http://www.usaweld.com/Parts-for-Mic...-625-parts.htm
    Also, Weldmart.com has them.
    http://www.weldmart.com/store/RTS-4700.htm

    For a cheap source as good as or better than what you found for the future:
    http://www.ebay.com/itm/10pcs-Tips-1...item5d2f944ffc

    You can get a rolling standoff from us for that torch.

    A thing about those consumables...They probably won't have the wear life...because they are made from inferior chinese recycled copper which has a high tin content which wears much faster. The ones we send with the torch are genuine trafimet, and our replacements use copper made and sourced from Finland...There's a big difference in wear.
    I did a search and that was what I found so I bought them.
    I can't get the USAweld link to work?!?

    I definitely like the drag tips and how they work so in the future I'll try some other sources. So what's up with that seller on Ebay?
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  6. #6

    Default

    I was thinking that was a little pricey for those consumables!
    Lincoln Eagle Engine Drive
    Everlast MTS 250
    Everlast Power Tig 225lx
    HTP Mig 2400
    Everlast Power Plasma 60C --> Just need to finish my CNC Plasma Table!
    Miller Spectrum 375 Extreme Plasma cutter
    Victor cutting torch
    HF 20 Ton Shop Press
    HF 4x6 Band Saw
    HF Air Compressor
    Northern Tool Drill Press


    www.murphywelding.com

  7. #7

    Default

    I bought some from this place better deal http://www.ebay.com/itm/320933592011...84.m1439.l2649
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  8. #8

    Default

    Quote Originally Posted by Rodsmachineshop View Post
    I bought some from this place better deal http://www.ebay.com/itm/320933592011...84.m1439.l2649
    WOW man... I really got screwed!!

    That's an awesome package for the price
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  9. Default

    You can always tell the originals from the copy,s as they are marked similar to this.

    Obviously i can not really be 100% sure about this but i firmly believe the Supplier that produces these is located in Wenzhou ( i only know of 2 suppliers for this drag tip in China)
    Interestingly Wenzhou is very close to Wenling . What makes Wenling somewhat infamous is it is one of three major centres for used electronics to be dismantled and parts recycled.

    You get of the train in Wenling and right away you can just feel the difference in both the soroundings and air quality and it is one of those depressing places that you come across and yet you can not really say why it makes you feel this way.
    I only spent 4 hours there but i can tell you i was very happy to leave. The sad thing is i will likely be back there fairly soon to visit another potential supplier.
    As for the consumables. I am pretty sure if i dug through some old files i could find pictures of the place producing them. I often use my Camera as a help along with recorder for keeping track of things i want to look into further.
    If i am correct the quality was rejected by us some time ago and we opted to use both original and another supplier that is in fact probably a little better wearing than the original.

    You really need to contact San Fran and tell them to order these Drag tips for you in the future as i can quarentee the quality will be superior.
    Cheers
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	A81 PICTIP 001.JPG 
Views:	660 
Size:	55.4 KB 
ID:	7691  
    EVERLAST CANADA
    www.everlastwelders.ca
    www.titanwinches.com

    905 637 1637

  10. #10

    Default

    Quote Originally Posted by Titan winch View Post
    You can always tell the originals from the copy,s as they are marked similar to this.

    Obviously i can not really be 100% sure about this but i firmly believe the Supplier that produces these is located in Wenzhou ( i only know of 2 suppliers for this drag tip in China)
    Interestingly Wenzhou is very close to Wenling . What makes Wenling somewhat infamous is it is one of three major centres for used electronics to be dismantled and parts recycled.

    You get of the train in Wenling and right away you can just feel the difference in both the soroundings and air quality and it is one of those depressing places that you come across and yet you can not really say why it makes you feel this way.
    I only spent 4 hours there but i can tell you i was very happy to leave. The sad thing is i will likely be back there fairly soon to visit another potential supplier.
    As for the consumables. I am pretty sure if i dug through some old files i could find pictures of the place producing them. I often use my Camera as a help along with recorder for keeping track of things i want to look into further.
    If i am correct the quality was rejected by us some time ago and we opted to use both original and another supplier that is in fact probably a little better wearing than the original.

    You really need to contact San Fran and tell them to order these Drag tips for you in the future as i can quarentee the quality will be superior.
    Cheers
    Mine look different then the picture you posted.... I'm headed to San Fran for Labor day weekend so maybe I could just drop in and get some!!
    PowerTig 250EX
    Power I-MIG 200
    Power Plasma 50
    It's what you learn, After you know it all, that counts!

  11. #11

    Default

    have to read get only 5 each for that price . guy was cool he sent me 3 tips and 3 electrodes for the the price to try out . mine look like this Click image for larger version. 

Name:	$(KGrHqJ,!iYE-TD)Gp9nBPwlyfC1QQ~~60_12.JPG 
Views:	689 
Size:	44.6 KB 
ID:	7692
    Last edited by Rodsmachineshop; 08-22-2012 at 04:01 PM.
    EVERLAST 250 EX , EVERLAST I-MIG 205 , EVERLAST spool gun NOW have 2 EVERLAST POWER PLASMA 50 plasma cutter's , LINCOLN 175HD MIG WELDER , VICTOR TORCH SET and many more tools to many to list

  12. #12

    Default

    Quote Originally Posted by CGCINC View Post
    I did a search and that was what I found so I bought them.
    I can't get the USAweld link to work?!?

    I definitely like the drag tips and how they work so in the future I'll try some other sources. So what's up with that seller on Ebay?
    Link is working for me. Just google it. Very reputable people.

  13. #13
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    What is the life difference between the good tips and the recycled ones? Is the quality of the cut the same when both are new? In a production environment or some field work where tip changing time might be an issue, I can see having the best quality. But for light use, all I really care about is cost per inch of cut. If the cheap ones have a better ROI, what do I care for parts that will be used up no matter what. It took me a long time to learn this, but sometimes "good enough", is.
    Long arc, short arc, heliarc and in-the-dark!

  14. #14

    Default

    Duncan has always leaned to the the quality side (real Trafimet logo on them or good copies without (was is black wolf)). Those will last longer. I have use all ranges myself.

    I've found the cheap ones work well and for the price, it's like buying a harbor freight screw driver, when it's done you pitch it and no problem.

    $12 vs $40, I would try the $12, can not lie, but I bet the $40 last longer unless a scam.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  15. #15

    Default

    Quote Originally Posted by Rambozo View Post
    What is the life difference between the good tips and the recycled ones? Is the quality of the cut the same when both are new? In a production environment or some field work where tip changing time might be an issue, I can see having the best quality. But for light use, all I really care about is cost per inch of cut. If the cheap ones have a better ROI, what do I care for parts that will be used up no matter what. It took me a long time to learn this, but sometimes "good enough", is.
    That's the way I see it. If the "good" parts cost three times what the lower quality ones do, they should last more than three times as long or there's no point. It takes less than sixty seconds to change tips.
    I've been using the cheap chinese consumables on a P80 torch and they have performed well for hobby work.
    2013 250EX : SSC Pedal : I-MIG 250P 20' Profax gun : Power Plasma 60 p80 torch : 3M Speedglas 9100XX : Evolution Rage 3 DB cold saw

  16. #16

    Default

    Quote Originally Posted by Rambozo View Post
    What is the life difference between the good tips and the recycled ones? Is the quality of the cut the same when both are new? In a production environment or some field work where tip changing time might be an issue, I can see having the best quality. But for light use, all I really care about is cost per inch of cut. If the cheap ones have a better ROI, what do I care for parts that will be used up no matter what. It took me a long time to learn this, but sometimes "good enough", is.
    From what I have personally experienced, anywhere between 2 to 4 times as long.

  17. #17

    Default

    Sorry to thread jack but do these fit on the Power Pro 205 Plasma torch.
    Brandon Raineri
    The Pennsylvania State University
    Studying Industrial Engineering

    Everlast PowerPro 205
    Everlast I-Mig 200
    SpeedGlas 9100x
    Milwaukee 14" Dry Cut Saw
    Craftsman 6"x48" Belt Sander with 9" Disc Sander

  18. #18
    Join Date
    May 2012
    Location
    Disneyland
    Posts
    2,663

    Default

    Quote Originally Posted by scootarida1 View Post
    Sorry to thread jack but do these fit on the Power Pro 205 Plasma torch.
    If you have the S45 torch.
    Long arc, short arc, heliarc and in-the-dark!

  19. #19

    Default

    Quote Originally Posted by scootarida1 View Post
    Sorry to thread jack but do these fit on the Power Pro 205 Plasma torch.
    This is the S45

    http://trafimetgroup.com/en/products...s45-torch.html
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  20. #20

    Default

    Anyone have measurements of drag tips for the Supercut 50P, I am going to a friends this weekend and going to sort threw 300-400 pounds of tips nozzles ect.I have a general idea of the what they look like just need some dia length ect.
    PowerTig 200DX
    Supercut 50P
    PowerTig Micro 185 SOLD GREAT MACHINE
    Millermatic 200
    Miller Thunderbolt
    Jet 1340 Lathe
    Jet 20" Drill Press
    Jet 12" Wet Band Saw
    Kalamazoo H7 Bandsaw
    Forward 12,000 lb 4 Post Lift

Similar Threads

  1. Drag tips for PT-60/iPT60
    By Gunther in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 09-04-2017, 03:18 PM
  2. Recieved my 2013 250EX today!
    By xalky in forum TIG Welding (GTAW/GTAW-P)
    Replies: 2
    Last Post: 03-08-2013, 01:43 PM
  3. Looking for drag tips for the S45 torch?
    By CGCINC in forum Everlast Plasma Cutters (PAC)
    Replies: 1
    Last Post: 08-14-2012, 02:15 AM
  4. recieved the powerarc 200
    By bobwills in forum Customer Testimonials
    Replies: 13
    Last Post: 11-04-2011, 11:46 PM
  5. Recieved my updated PP205
    By NRM in forum Multi-Process Units (TIG,Stick,Plasma/MIG,TIG,Stick Combo units)
    Replies: 16
    Last Post: 06-13-2011, 03:48 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •