    I have half a can of 7018 some one me that has developed a coating of white powerdery stuff. What can I do to get them usable?
    Charlie

    Everlast 225 LX
    Everlast PP 50

    HF 130 TIG/90 ARC
    HF 90 fluxcore

    ATX MIG (don't ask)

  2. #2

    Default

    You could try to rebake them, but they're tedious to do properly, and it is likely the flux will crack off.

    You'll be better to use them for practice, or throw them out/recycle them.

Similar Threads

  1. Preheating in an oven
    By dsthompson in forum General Welder Questions
    Replies: 1
    Last Post: 03-28-2018, 07:30 PM
  2. Harbor freight 9 dollar torch
    By RCnMo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 01-03-2012, 05:57 AM
  3. Powder Coating Oven project
    By DAC45 in forum Other Custom Fabrications
    Replies: 19
    Last Post: 10-13-2011, 05:18 AM
  4. Powder Coating Oven
    By acourtjester in forum Other Custom Fabrications
    Replies: 4
    Last Post: 07-01-2011, 09:59 PM
  5. Got my eye on a small rod oven
    By Haywire in forum General Welding Questions
    Replies: 8
    Last Post: 06-10-2011, 10:06 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •