    Don't try silica gel/bags as it is designed to absorb moisture. Anytime it is exposed to any moisture it tries to retain it. However, after it has fully absorbed all that it can, it allows the moisture it can't, to absorb into the rods. Any small cracks or leaks will saturate the silica beyond its capabilities and it constantly will continue to absorb moisture into your storage can. It acts like a magnet constantly sucking in moisture. I ruined a can of 9018, 11018 trying to do this.
    Last edited by jsclark4500; 04-14-2011 at 07:45 PM.

Similar Threads

  1. Preheating in an oven
    By dsthompson in forum General Welder Questions
    Replies: 1
    Last Post: 03-28-2018, 07:30 PM
  2. Harbor freight 9 dollar torch
    By RCnMo in forum TIG Welding (GTAW/GTAW-P)
    Replies: 5
    Last Post: 01-03-2012, 05:57 AM
  3. Powder Coating Oven project
    By DAC45 in forum Other Custom Fabrications
    Replies: 19
    Last Post: 10-13-2011, 05:18 AM
  4. Powder Coating Oven
    By acourtjester in forum Other Custom Fabrications
    Replies: 4
    Last Post: 07-01-2011, 09:59 PM
  5. Got my eye on a small rod oven
    By Haywire in forum General Welding Questions
    Replies: 8
    Last Post: 06-10-2011, 10:06 AM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •