    Hi, new to the site, well been a member for while but haven't posted till now. Just wanted to show you guys some of my practice peices on pulsed tig AC/DC of aluminum and SS on my powermaster 256. Never really did any pulse welding until I bought this machine because my work felt that it wasn't neccessary. Not bad for only 5 years experience. Will have more pictures later this week on actual jobs I need to do on aluminum.

    All aluminum welds were done with a 2% 3/32 ceriated tungsten sharpended to a blunt point and was 1/8" 4000 series AL. The ceriated works best on this machine for all AC/DC welding based on all the tungstens I have tested (2% thoriated, 1.5% lanthanated, pure, and zirconium). Plan to eventually put a water cooler on this machine to use either a wp20 or my wp24w torch.
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	100_0434.jpg 
Views:	877 
Size:	37.1 KB 
ID:	237   Click image for larger version. 

Name:	100_0438.jpg 
Views:	901 
Size:	41.4 KB 
ID:	238   Click image for larger version. 

Name:	100_0441.jpg 
Views:	866 
Size:	34.6 KB 
ID:	239  

  2. #2

    Default

    Welcome to the forum. Nice looking welds. What type of projects are you in to?
    Wayne

  3. Default

    my biggest hobby is bulding parts for sport ATVs, but looking into the supermoto also. expample: exhausts (TI and SS), control arms, custom gas tanks, modified swingarms, etc. If you want I can post more pictures of parts I have made in the past with my old syncrowave 250

  4. #4

    Default

    Sure, we love pictures!
    Wayne

  5. #5

    Default

    Quote Originally Posted by cdale2002 View Post
    Hi, new to the site, well been a member for while but haven't posted till now. Just wanted to show you guys some of my practice peices on pulsed tig AC/DC of aluminum and SS on my powermaster 256. Never really did any pulse welding until I bought this machine because my work felt that it wasn't neccessary. Not bad for only 5 years experience. Will have more pictures later this week on actual jobs I need to do on aluminum.

    All aluminum welds were done with a 2% 3/32 ceriated tungsten sharpended to a blunt point and was 1/8" 4000 series AL. The ceriated works best on this machine for all AC/DC welding based on all the tungstens I have tested (2% thoriated, 1.5% lanthanated, pure, and zirconium). Plan to eventually put a water cooler on this machine to use either a wp20 or my wp24w torch.
    I have used thoriated with good results as well...not to say ceriated isn't a premium solution, but, that thoriated is a more than adequate starting point for aluminum as well, but a lot depends upon your settings. The factory torch looks like it does a pretty good job to me, but I do know what you mean. The trafimet is not everyone's choice. But if some were to buy a miller, many end up changing their torch as well.

  6. #6

    Default

    cdale2002,

    Nice welds. Welcome to the forum and thanks for posting.

    Will pick up some ceriated 3/32" next time I do the 200lbs bottle lift.. Normally use 2% thoriated but always open to try something new.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

  7. Default

    the stock torch does do fine but for the amount of aluminum I may end up doing, a watercooled torch is a must have. Just did a small job on some aluminum as you see in the pic (this wasn't welded on my PM256 but the millers we have at work), but the one I did on my PM256 its 2 inches shorter and looked just as nice. The torch was so hot after doing the big center plate on one side that you almost couldn't touch the torch and had to let it cool down
    Attached Thumbnails Attached Thumbnails Click image for larger version. 

Name:	cdale27+4.5.jpg 
Views:	718 
Size:	33.9 KB 
ID:	240   Click image for larger version. 

Name:	cdale27+4.3.jpg 
Views:	751 
Size:	33.1 KB 
ID:	241  

  8. #8

    Default

    We have a water cooled torch available and a water cooler. Call Alex and he will give you a deal.

  9. #9
    Join Date
    Jul 2010
    Location
    Port Saint Lucie , Florida
    Posts
    85

    Default

    I thought the 256 comes with a water cooled torch ?
    Gary

  10. Default

    My 256 did come with a water cooled torch.

  11. #11

    Default

    In January it was a option (when this thread started), now they come with water cooled torches.
    Mike R.
    Email: admineverlast@everlastwelders.com
    www.everlastgenerators.com
    www.everlastwelders.com
    877-755-9353 x203
    M-F 12 - 7PM PST
    FYI: PP50, PP80, IMIG-200, IMIG-250P, 210EXT and 255EXT.

Similar Threads

  1. Pulsed Arc Welding?
    By scootarida1 in forum Stick Welding (SMAW)
    Replies: 5
    Last Post: 12-06-2012, 01:04 PM
  2. Excellent Pulsed TIG article
    By earla in forum TIG Welding (GTAW/GTAW-P)
    Replies: 1
    Last Post: 08-25-2012, 01:49 AM
  3. Question about Pulsed Mig Process
    By Oxide00 in forum General Welder Questions
    Replies: 11
    Last Post: 03-20-2011, 12:23 AM
  4. 250P pulsed mig
    By Metalux in forum MIG Welding (GMAW/GMAW-P/FCAW)
    Replies: 7
    Last Post: 02-22-2010, 02:55 PM
  5. Purchased 200 ACDC Pulsed
    By wallnut in forum Customer Testimonials
    Replies: 2
    Last Post: 05-01-2009, 12:54 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •